GA-11 × 1 silicone roba sx na-akpụzi nke ọma na -eme ka ezigbo mgbochi na-acha odo odo na-acha odo odo (HCR)

Ngwa: A na-achọ ihe na-acha odo odo na-acha odo odo, kaa akara ngwaahịa
  • Ga-11 × 1

  • Herchy

;
wdg

Nwalee: 1% nke curninglọnga (50% mado nke DBPMH na Silicone chịngọm), 175 Celsius x 5MIN x 15MPA.


Poramita ngwaahịa
Ihe emeputara ohuru Ga-11331
Ga-1141 Ga-1151 Ga-1161 Ga-1171 Ga-1181
Mputa Transfecent
Williamplity
115
150
205
240
280
260
Ihe siri ike (Shorea)
30
40
50
60
70
80
Nnọọ (G / CM3) 1.10
1.12
1.16
1.19
1.22
1.23
Tensilestrreth (MPA)

7
8.5
8.5
8.5
7.5
7.5
Elongation (%) 700
550
450
400
300
200
Condstred (KN / M) 15
19
20
19
19
19





Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: Mba.33, Lane 159, Taiye Road, District FENDXIE, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai rọtchy rọba Co., LTD. Pe |   Amụma Nzuzo | Nkwado site na Ndukwa.