Tel: +86 15221953351 E-imeri: info@herchyrubber.com
Please Choose Your Language
IBICURUZWA
Uri hano: Murugo » Ibicuruzwa » Rubber » VMQ Silicone » GA-11 × 1 Silicone Rubber Fr Molding hamwe na Propery nziza yo kurwanya umuhondo (HCR)

imizigo

Sangira kuri:
buto yo kugabana kuri facebook
buto yo kugabana twitter
umurongo wo kugabana umurongo
wechat kugabana buto
guhuza kugabana buto
buto yo kugabana
buto yo kugabana whatsapp
buto yo kugabana

GA-11 × 1 Silicone Rubber Fr Kubumba hamwe na Propery nziza yo kurwanya umuhondo (HCR)

buto yohejuru, ibicuruzwa bifunga kashe nibindi.
  • GA-11 × 1

  • Herchy

Gushyira mu bikorwa: kurwanya umuhondo ibisabwa
bya

Ikizamini: 1% yumuti ukiza (50% paste ya DBPMH mumase ya silicone), 175 ° x 5min x 15MPa.


Ibipimo byibicuruzwa
Ibicuruzwa GA-11331
GA-1141 GA-1151 GA-1161 GA-1171 GA-1181
Kugaragara Birasobanutse
Yamamoto
115
150
205
240
280
260
Gukomera (ShoreA)
30
40
50
60
70
80
Ubucucike (g / cm3) 1.10
1.12
1.16
1.19
1.22
1.23
Imbaraga zingana (MPa)

7
8.5
8.5
8.5
7.5
7.5
Kurambura (%) 700
550
450
400
300
200
Imbaraga zamarira (kN / m) 15
19
20
19
19
19





Mbere: 
Ibikurikira: 

LINKS

IBICURUZWA BYACU

AMAKURU

Ongeraho: No.33, Umuhanda 159, Umuhanda wa Taiye, Akarere ka Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Uburenganzira     2023 Shanghai Herchy Rubber Co., Ltd. Ikarita |   Politiki Yibanga | Inkunga Na Kurongora.