GA-11×1 Silicone Rubber Fr Molling with Good Property Anti-kōwhai (HCR)

Taupānga: Ko nga whakaritenga o te kowhai kowhai o nga patene teitei, te hiri hua me etahi atu waahanga matua: he pai nga taonga anti-kowhai, he maamaa teitei, he tino pai te mahi, ka tukuna te whakamotuhēhēnga o RoHS, REACH, me te FDA
  • GA-11×1

  • Herchy

Availability:
Rahi:

Whakamatau: 1% o te kaihoko whakaora (50% te whakapiri o te DBPMH i roto i te kapia silicone), 175° x 5min x 15MPa.


Tawhā hua
Hua GA-11331
GA-1141 GA-1151 GA-1161 GA-1171 GA-1181
Te ahua Puatarangi
Williamplasticity
115
150
205
240
280
260
Maama (ShoreA)
30
40
50
60
70
80
Kiato(g/cm3) 1.10
1.12
1.16
1.19
1.22
1.23
Te kaha (MPa)

7
8.5
8.5
8.5
7.5
7.5
Whakaroa(%) 700
550
450
400
300
200
Te Roimata (kN/m) 15
19
20
19
19
19





Tōmua: 
Panuku: 

NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.