GA-11×1
Herchy
| Disponibilite: | |
|---|---|
| Kantite: | |
Tès: 1% nan ajan geri (50% keratin nan DBPMH nan jansiv silikon), 175 ° x 5min x 15MPa.
| Paramèt pwodwi | ||||||
| Pwodwi | GA-11331 |
GA-1141 | GA-1151 | GA-1161 | GA-1171 | GA-1181 |
| Aparans | Translusid | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
260 |
| Dite (ShoreA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Dansite (g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.23 |
| Fòs traction (MPa) |
7 |
8.5 |
8.5 |
8.5 |
7.5 |
7.5 |
| elongasyon (%) | 700 |
550 |
450 |
400 |
300 |
200 |
| Fòs chire (kN/m) | 15 |
19 |
20 |
19 |
19 |
19 |