GA- 11×1
Earcach
| Infhaighteacht: | |
|---|---|
| Cainníocht: | |
Tástáil: 1% den ghníomhaire leigheas (50% de DBPMH a ghreamú i guma silicone), 175° x 5min x 15MPa.
| Paraiméadair táirge | ||||||
| Táirge | GA- 11331 |
GA- 1141 | GA- 1151 | GA- 1161 | GA- 1171 | GA-1181 |
| Dealramh | Tréshoilseach | |||||
| Williamplasticity |
115 |
150 |
205 |
240 |
280 |
260 |
| Cruas (ShoreA) |
30 |
40 |
50 |
60 |
70 |
80 |
| Dlús(g/cm3) | 1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.23 |
| Neart teanntachta (MPa) |
7 |
8.5 |
8.5 |
8.5 |
7.5 |
7.5 |
| Fadú(%) | 700 |
550 |
450 |
400 |
300 |
200 |
| neart cuimilt (kN/m) | 15 |
19 |
20 |
19 |
19 |
19 |