GA-2610
Herchy
| Avanoa: | |
|---|---|
| Aofa'i: | |
Su'ega: fua faatatau A/B ole 1:1, 130°C x 5min x 15MPa
| Fa'asologa o oloa | |||||||||
| Oloa | GA-2610 | GA-2620 | GA-2630 | GA-2640 | GA-2650 | GA-2660 | GA-2670 | GA-2680 | |
| Fa'aaliga | Malamalama | ||||||||
| Viscosity(Pa.s) |
1500 | 2000 | 2500 | 3000 | 3500 | 4000 |
4000 |
5500 |
|
| Malosi (ShoreA) | 10 | 20 | 30 | 40 | 50 |
60 |
70 |
80 |
|
| Malosi (g/cm3) | 1.08 | 1.10 | 1.10 | 1.11 | 1.12 |
1.13 |
1.14 |
1.15 |
|
| Malosi fa'amalosi (MPa) | 4.5 |
6.5 |
7.5 |
9.5 |
10.0 |
10.0 |
9.5 |
9.0 |
|
| Fa'atele(%) | 900 | 880 | 800 | 700 | 550 |
450 |
350 |
350 |
|
| Malosi o loimata (kN/m) | 8 | 12 | 15 | 25 | 35 |
35 |
30 |
30 |
|
| Linearshrinkage(%) | 2.3 | 2.1 | 2.1 | 2.1 | 2.0 |
2.0 |
2.0 |
2.0 |
|
| Tu'u atu(%) | 90 |
90 | 90 | 90 | 90 | 90 | 90 | 90 | |