Fluoroelastomer -FKM/FPM

Fluoroelastomer o se polymer elastomer synthetic o lo'o i ai atoms fluorine i luga o le carbon atoms o le filifili autu po'o le filifili itu. O le faʻaofiina o atoms fluorine e maua ai le paʻu sili ona lelei le vevela, faʻamaʻi faʻamaʻi, faʻamaʻi suauʻu, faʻamaʻi faʻamaʻi ma le malosi o le ea, ma e faʻaaogaina lautele i vaalele, vaalele, taʻavale, suauu ma meafale.
Avanoa:
Aofaiga:

Fluoroelastomer pa'u fa'afefiloi-FKM


FKM pa'u oloa e sili atu le maualuga o le tete'e o le vevela, kemisi corrosion tete'e, suauu tetee, lelei tumau deformation faatinoga, afi tetee ma le kesi permeability.


Fluoroelastomer e masani ona faʻaaogaina i le maualuga ma le maualalo o le vevela faʻamaufaʻailoga, masini masini ma meafaigaluega, masini vailaʻau, taavale, vaalele ma isi fanua.


O le Herchy Rubber o lo'o i ai se 'au R&D fa'apolofesa e fa'afetaui mana'oga fa'apitoa a tatou tagata fa'atau.

●Bisphenol vulcanization faiga ma peroxide vulcanization faiga

●Atiae ma gaosia oloa mo le faʻapipiʻiina, tui, extrusion ma isi auala gaosi.

●Customize fluoroelastomer compound ma le maaa 50-90 tikeri, lanu eseese ma talosaga e tusa ai ma manaoga o tagata faatau.


Herchy Ituaiga Vulcanization mea e maua ai le fluorine viscosity Mooney Malosi Malosi fa'asa Elongation i le malologa TR10 Seti fa'amalosi Fa'atatauga Uiga







200℃*72h ASTM D395 Ituaiga B
Vasega % ML(1+10)121℃ g/cm3 Mpa % ℃ %
FKM-65B20 Bisphenol 65.9 20 1.8 12.3 170 -17 17 O-mama ;Kesi Seti fa'amalosi maualalo;
Lelei lelei;
FKM-65B40 Bisphenol 65.9 40 1.81 14.3 180 -17 16 O-mama ;Kesi Malosi fa'ainisinia maualuga;
Seti fa'amaulalo maualalo
FKM-65B60 Bisphenol 65.9 60 1.81 15.5 180 -17 16 O-mama ;Kesi Malosi fa'ainisinia maualuga;
Seti fa'amaulalo maualalo
FKM-68B40 Bisphenol 68.5 40 1.85 14.3 220 -14 26 O-mama ;Kesi Lelei lelei;
E sili atu le tete'e atu i fa'asalalauga kemikolo;
Maualuluga le vevela
FKM-68B60 Bisphenol 68.5 60 1.85 16.2 200 -14 26 O-mama ;Kesi Malosi fa'ainisinia maualuga;
Lelei le tetee atu i fa'asalalauga kemisi;
maualuga le vevela
FKM-65B30S Bisphenol 65.9 30 1.80 15.0 190 -20 21 Oloa fa'alafoa'i, oloa tui, oloa fa'ameamea Tete'e maualalo vevela;
Malosi fa'ainisinia maualuga
;
FKM-70P30 Peroxide 70 30 1.9 18.5 220 -7 36 Oloa fa'alafoa'i, oloa tui, oloa fa'ameamea Lelei lelei;
Sili atu acid ma alkaline tetee;
E sili atu le tete'e atu i fa'asalalauga kemikolo;
Maualuluga le vevela
FKM-68P45 Peroxide 68 45 1.85 16.5 280 -16 36 Oloa fa'alafoa'i, oloa tui, oloa fa'ameamea Lelei lelei;
Sili atu acid ma alkaline tetee;
E sili atu le tete'e atu i fa'asalalauga kemikolo;
Maualuluga le vevela


1. Faamaufaailoga

Fa'ailoga afi

O la'u faamaufaailoga

Fa'amaufa'ailoga vaila'au

Fa'amaufa'ailoga ausa fa'avevela

Fufulu fa'amau fa'amau

ipu pa'u

Faamaufaailoga suauu


2. Faagaau

Fa'agaau pa'u maualuga vevela

Fa'agaau suauu ta'avale

Fa'agaau suauu vaalele

Paipa fa'atasi


3. Uaea ma uaea

O le uaea ma le uaea e faia i le fluoroelastomer e fefiloi lelei ma e lelei mea e fa'a'ese'ese ai


4. Fiberglass lipine

O le vevela maualuga o le 300 ℃ ma le faʻamaʻi faʻamaʻi


Muamua: 
Sosoo ai: 

SO'OGA VAIVAI

OA TATOU Oloa

FA'AMATALAGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.