GA-2033 Fingotra Silicone fanosotra tena (LSR)

Fampiharana: mety amin'ny famokarana kojakoja fiara, plug, sns.
Ny endri-javatra lehibe: hery avo, fananana mandeha ra menaka tsara.
  • GA-2033

  • Herchy

Availability:
Quantity:

Fitsapana: tahan'ny A/B amin'ny 1:1, 130°C x 5min x 15MPa

Masontsivana vokatra
vokatra GA-2033
GA-2043 GA-2053 GA-2045
Bika Aman 'endrika Translucent
Viscosité (Pa.s)
2000 3000 4000 3500
Hardness (ShoreA) 30 40 50
40
Hateza (g/cm3) 1.10 1.12 1.14 1.13
Henjana (MPa) 6.5
8.0
9.5
7.5
Elongation(%) 650 550 500 550
Herin-dranomaso (kN/m) 13 20 27
21
Linearshrinkage(%) 1.8 1.8 1.8 1.8
Set famatrarana 175 x 22H (%) -
-
-
20










teo aloha: 
Manaraka: 

ROHINY HAINGANA

NY PRODUKY

ANTSIPIRIANY IFANDRAISANA

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Politika momba ny fiainana manokana | Support By Leadong.