GA-2340 Molding Fanampiny-manasitrana Silicone fingotra (LSR)

Fampiharana: Azo ampiharina amin'ny famokarana lasitra vita amin'ny resin thermosetting, toy ny resin'ny epoxy sns Endri-javatra manan-danja: hery avo, fanasitranana haingana, stab 小ty, be dia be ny fanonganana.
  • GA-2340

  • Herchy

Availability:
Quantity:

Fitsapana: AB ratio 10:1 na 1:1, 130'C x 5min x 15Mpa.

Masontsivana vokatra
vokatra GA-2340
GA-2341
Bika Aman 'endrika Translucent
A/Bratio A:B=10:1
A:B=1:1
Viscosité (Pa.s)
50/1 75/75
Hardness (ShoreA) 38 38
Hateza (g/cm3) 1.08 1.08
Henjana (MPa) 6.5
6.5
Elongation(%) 400 400
Herin-dranomaso (kN/m) 18 18
Linearshrinkage(%) 2.0
2.0












teo aloha: 
Manaraka: 

ROHINY HAINGANA

NY PRODUKY

ANTSIPIRIANY IFANDRAISANA

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Politika momba ny fiainana manokana | Support By Leadong.