Fluorosilicone Flexilis FV9200

Productum hoc uniforme mixtum fluorosilicone-substructio tenaces est, quod varias supplementa et fillers continet.
Superior princeps distrahentes vires et altum lacrima efficientiam.
Superbum oleum resistentia, resistentia solvens et resistentia calidi et gravis.
  • FV9200

  • Herchy

Availability:
Quantity:




Items


Indicatores

Grades

FV9240

FV9250

FV9260

Test Methodi / Aspectus

Lacteus albus translucens

Imprimis Gravitas/g/cm3

ASTM D792

1.42

1.44

1.45

Duritiam / shoreA

ASTM D2240

40

50

60

Distrahentes Fortitudo / MPa

ASTM D412

10.1

10.2

10.3

Prolongatio In Gaudete /%

ASTM D412

490

457

440

Lacrima fortitudo/KN/m

ASTM D624-B

35

42

43

Compressione Set (177℃*22h)

ASTM D395

11

11

12

* Calor Resistentia
225℃×72h

Duritiam mutationem / litus A

+3

+3

+2

Roboris distrahentes mutatio, %

-19

-16

-17

Prolongatio in mutatione intermissum, %

-14

-17

-18

Cibus C

Volumen Mutare/%

23℃/72h

ASTM D471

23

21

20

Sanatio Condition

0.7 DBPH, Press remedium: 170℃×15min,Post remedium: 200℃×4h


Commendatur actus:


Suadet utendi 0.6 ad 1 partem bisdipentae agentis chemici pro vulcanizatione (2,5-dimethyl-2,5-bis(tert-butylperoxy)hexane).


Customers debent eligere temperiem aptissimum et tempus medendi secundum magnitudinem ac modum medendi producti.


Product packaging:


Productum hoc periculosum non est, loco constat ex cardstock, plastica, et 10 chiliogrammata per sacculum, saccos 2 per pixidem.


Aevum repono:


Hoc productum facultatem frigidum habet, vitandus est sacculus ne laedatur in translatione vel utendo.


Serva in frigido, sicco ambitu cum pluteo vita XII mensium.

Previous: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.