Bata Roba Soles

Bata Roba Soles


Awọn ibọsẹ rọba jẹ awọn atẹlẹsẹ ti a fi ṣe roba, ati awọn ohun elo atẹlẹsẹ rọba le pin si roba adayeba tabi roba sintetiki. Anfani ti roba adayeba ni pe o jẹ rirọ pupọ, rirọ ti o dara julọ, o le ṣe deede si awọn ere idaraya pupọ, lati ṣe ipa ipa-mọnamọna, ṣugbọn aila-nfani naa tun han gbangba ti o jẹ resistance epo, ogbo osonu ati ogbo atẹgun gbona ko dara. Awọn bata idaraya inu ile julọ lo roba adayeba.

Ṣeduro:

EPDM:S537-3;S537-2;J-2070;J-2080;TER 6235;TER 4548;