Hydrogenated nitrile roba precompound ati yellow-HNBR
roba nitrile hydrogenated (HNBR tabi HSN) jẹ ọja ti hydrogenation ati ekunrere ti erogba-erogba meji mnu ni molikula pq ti nitrile roba, ki o tun npe ni gíga po lopolopo nitrile roba.
HNBR ni o ni idaabobo epo to dara (iduroṣinṣin ti o dara si epo epo, awọn lubricants, awọn nkan ti oorun didun); ati nitori eto ti o ni itara pupọ, o ni resistance ooru to dara, resistance kemikali ti o dara julọ (iduroṣinṣin ti o dara si Freon, acids ati alkalis), resistance osonu ti o dara julọ, ati resistance giga si ibajẹ ayeraye ni funmorawon; ni akoko kanna, HNBR tun ni agbara giga, iṣẹ ṣiṣe yiya. HNBR tun ni o ni ga agbara, ga yiya išẹ, o tayọ yiya resistance, bbl O jẹ ọkan ninu awọn roba pẹlu o tayọ ìwò išẹ.
Herchy Rubber ni ẹgbẹ imọ-ẹrọ ọjọgbọn kan pẹlu iriri ọlọrọ ni HNBR R&D. A le ṣe agbekalẹ awọn ọja fun awọn ohun elo oriṣiriṣi ni ibamu si awọn iwulo awọn alabara. Ati ki o gbadun ga rere ni China ati awọn aye.
| Herchy | Vulcanization iru | Acrylonitrile akoonu | Mooney iki | Lile | Agbara fifẹ | Elongation ni isinmi | IRM 903 iyipada iwọn didun | Funmorawon ṣeto | Ohun elo | Ohun kikọ |
| 150 ℃ * 72h | 150℃*72h ASTM D395 Iru B | |||||||||
| Ipele | % | ML (1+4)100℃ | Etikun A | Mpa | % | % | % | |||
| HNBR-S6035 | Efin | 35 | 50-100 | 60 | 17–24 | 300-500 | <20 | <60 | Awọn ọja ni ile-iṣẹ epo, | Nla elongation, Ti o dara ara-adhesiveness, Exllent processing |
| HNBR-S7035 | Efin | 35 | 50-100 | 70 | 17–24 | 300-500 | <20 | <60 | Awọn ọja ni oilfield ile ise, Automobile ile ise, igbanu |
Agbara rirẹ agbara, Resistance ara-Resistance, Exllent processing |
| HNBR-S8035 | Efin | 35 | 50-100 | 80 | 17–24 | 300-500 | <20 | <60 | Liluho paipu aabo fẹlẹfẹlẹ, Ppressure accumulators |
Idaabobo titẹ giga, Adhesiveness ti ara ẹni to dara |
| HNBR-S6043 | Efin | 43 | 50-100 | 60 | 17–24 | 300-500 | <10 | <60 | Idana ọkọ ayọkẹlẹ, Awọn ọja ni ile-iṣẹ epo |
Epo resistance, Exllent processing |
| HNBR-S7043 | Efin | 43 | 50-100 | 70 | 17–24 | 300-500 | <10 | <60 | Awọn ọja ni ile-iṣẹ epo, ile-iṣẹ ọkọ ayọkẹlẹ, |
Idaabobo epo, Agbara agbara agbara, Resistance ara ẹni to dara |
| HNBR-S8043 | Efin | 43 | 50-100 | 80 | 17–24 | 300-500 | <10 | <60 | Liluho paipu aabo fẹlẹfẹlẹ, Ppressure accumulators |
Idaabobo epo, Idaabobo titẹ giga, Imudara ara ẹni ti o dara |
| HNBR-P6035 | Peroxide | 35 | 50-100 | 60 | 17–24 | 200-350 | <20 | <30 | Ile-iṣẹ ọkọ ayọkẹlẹ, ile-iṣẹ iṣelọpọ ọkọ ofurufu |
Agbara otutu giga, sisẹ to gaju |
| HNBR-P7035 | Peroxide | 35 | 50-100 | 70 | 17–24 | 200-350 | <20 | <30 | Ikole ile ise, Engine gaskets, Eyin-oruka, edidi |
Agbara otutu giga, ṣeto funmorawon to dara |
| HNBR-P8035 | Peroxide | 35 | 50-100 | 80 | 17–24 | 200-350 | <20 | <30 | Awọn paipu liluho, Awọn ikojọpọ titẹ, |
Agbara titẹ giga, Idaabobo iwọn otutu giga |
| HNBR-P6043 | Peroxide | 43 | 50-100 | 60 | 17–24 | 200-350 | <10 | <30 | Idana ọkọ ayọkẹlẹ ati awọn eto Lubrication | Epo resistance, Exllent processing, Ti o dara funmorawon ṣeto |
| HNBR-P7043 | Peroxide | 43 | 50-100 | 70 | 17–24 | 200-350 | <10 | <30 | Engine gaskets, Eyin-oruka, edidi, igbanu |
Epo resistance, Ti o dara funmorawon ṣeto, Exllent processing |
| HNBR-P8043 | Peroxide | 43 | 50-100 | 80 | 17–24 | 200-350 | <10 | <30 | Liluho oniho, Ipa accumulators |
Idaabobo epo, Idaabobo titẹ giga, Idaabobo otutu otutu |
1. Triangular igbanu
2. Gbigbọn Isolators
3.
Awọn edidi
4. Ooru sooro pipe
5.
Liluho Idaabobo apoti
6. Pisitini fun awọn ifasoke ẹrẹ
7.
Lilẹ gaskets fun awọn Oko ile ise
8. Awọn edidi fun awọn ibudo agbara
9.
Awọn okun hydraulic
10. Hydraulic edidi
11. USB sheaths fun agbara ibudo
12. Titẹ sita ati fabric rollers
13. edidi fun Aerospace
14. Awọn ideri
15.Fuel àpòòtọ