GA-26X0 Sihin-giga ati Agbara LSR (LSR)

Ohun elo: o dara fun iṣelọpọ awọn ohun elo ibi idana giga-giga, awọn ipese odo, awọn ipese ọmọ, ati bẹbẹ lọ.
Awọn ẹya pataki: agbara giga, akoyawo giga, ipele ounjẹ, kọja ijẹrisi ti RoHS, REACH, FDA ati LFGB.
  • GA-2610

  • Herchy

Wiwa:
Opoiye:

Idanwo: Ipin A/B ti 1: 1, 130°C x 5min x 15MPa



Ọja sile


Ọja GA-2610 GA-2620 GA-2630 GA-2640 GA-2650 GA-2660 GA-2670 GA-2680
Ifarahan Sihin



Igi (Pa.s)
1500 2000 2500 3000 3500 4000
4000
5500
Lile ( ShoreA) 10 20 30 40 50
60
70
80
Ìwúwo (g/cm3) 1.08 1.10 1.10 1.11 1.12
1.13
1.14
1.15
Agbara fifẹ (MPa) 4.5
6.5
7.5
9.5
10.0
10.0
9.5
9.0
Ilọsiwaju(%) 900 880 800 700 550
450
350
350
Agbara omije (kN/m) 8 12 15 25 35
35
30
30
Laini idinku(%) 2.3 2.1 2.1 2.1 2.0
2.0
2.0
2.0
Gbigbe(%) 90
90 90 90 90 90 90 90




Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. Maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.