GA-2340 Imudanu Afikun-itọju Liquid Silikoni roba (LSR)

Ohun elo: Wulo lati ṣe agbejade apẹrẹ iṣẹ ọna ti resini thermosetting, gẹgẹbi, resini iposii ati bẹbẹ lọ Awọn ẹya pataki: agbara giga, imularada iyara, onisẹpo stab, awọn nọmba giga ti yiyi.
  • GA-2340

  • Herchy

Wiwa:
Opoiye:

Idanwo: ipin AB ti 10:1 tabi 1:1, 130'C x 5min x 15Mpa.

Ọja sile
Ọja GA-2340
GA-2341
Ifarahan Translucent
A/Blatio A:B=10:1
A:B=1:1
Igi (Pa.s)
50/1 75/75
Lile ( ShoreA) 38 38
Ìwúwo (g/cm3) 1.08 1.08
Agbara fifẹ (MPa) 6.5
6.5
Ilọsiwaju(%) 400 400
Agbara omije (kN/m) 18 18
Laini idinku(%) 2.0
2.0












Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. maapu aaye |   Asiri Afihan ~!phoenix_var191_1!~ Leadong.