Kɔrɔbɔli : A/B hakɛ ye 1 :1 ye, 130°C x 5min x 15MPa
| Fɛn dilannenw ka paramɛtiriw | |||||
| Ka kɛ | GA-2033 ye |
GA-2043 ye | GA-2053 ye | GA-2045 ye | |
| Yecogo | Translucent (yɔrɔ jɛlen) ye | ||||
| Viscosité(Pa.s) ka . |
2000 | 3000 | 4000 | 3500 | |
| Gɛlɛya (KɔgɔjidaA) . | 30 | 40 | 50 |
40 |
|
| Densité(g/cm3) ye. | 1.10 | 1.12 | 1.14 | 1.13 | |
| Sɛgɛsɛgɛli fanga (MPa) . | 6.5 |
8.0 |
9.5 |
7.5 |
|
| Janya(%) . | 650 | 550 | 500 | 550 | |
| Ɲɛjibɔ fanga (kN/m) . | 13 | 20 | 27 |
21 | |
| Linearshrinkage(%) Bamako, Mali. | 1.8 | 1.8 | 1.8 | 1.8 | |
| 175 x 22H (%) ye 175 x 22H ye. | - |
- |
- |
20 |
|