GA-2033
Herhhik
Kättesaadavus: | |
---|---|
kogus: | |
Test: A/B suhe 1: 1, 130 ° C x 5min x 15MPa
Tooteparameetrid | |||||
Toode | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Välimus | Poolläbipaistev | ||||
Viskoossus (Pa.S) |
2000 | 3000 | 4000 | 3500 | |
Kõvadus (Shorea) | 30 | 40 | 50 |
40 |
|
Tihedus (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Tõmbetugevus (MPA) | 6.5 |
8.0 |
9.5 |
7.5 |
|
Pikenemine (%) | 650 | 550 | 500 | 550 | |
Pisaratugevus (kn/m) | 13 | 20 | 27 |
21 | |
LinearSHINKINGE (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
Kompressionikomplekt 175 x 22H (%) | - |
- |
- |
20 |
Test: A/B suhe 1: 1, 130 ° C x 5min x 15MPa
Tooteparameetrid | |||||
Toode | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Välimus | Poolläbipaistev | ||||
Viskoossus (Pa.S) |
2000 | 3000 | 4000 | 3500 | |
Kõvadus (Shorea) | 30 | 40 | 50 |
40 |
|
Tihedus (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Tõmbetugevus (MPA) | 6.5 |
8.0 |
9.5 |
7.5 |
|
Pikenemine (%) | 650 | 550 | 500 | 550 | |
Pisaratugevus (kn/m) | 13 | 20 | 27 |
21 | |
LinearSHINKINGE (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
Kompressionikomplekt 175 x 22H (%) | - |
- |
- |
20 |