GA-2033
HERCHY .
Disponibilité: | |
---|---|
Quantité: | |
Momekano: A/B Ratio ya 1 :1, 130°C x 5min x 15mpa
Ba paramètres ya produit . | |||||
Eloko | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Komonana | Translucide . | ||||
Viscosité(pa.s) . |
2000 | 3000 | 4000 | 3500 | |
Bokasi ya makasi (Sorea) . | 30 | 40 | 50 |
40 |
|
Densité(g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Bokasi ya kokangama (MPA) . | 6.5 |
8.0 |
9.5 |
7.5 |
|
Elongation(%) . | 650 | 550 | 500 | 550 | |
Bokasi ya mayi ya miso (KN/M) . | 13 | 20 | 27 |
21 | |
linearshrinkage(%) . | 1.8 | 1.8 | 1.8 | 1.8 | |
CompressionSet 175 x 22h (%) . | - |
- |
- |
20 |
Momekano: A/B Ratio ya 1 :1, 130°C x 5min x 15mpa
Ba paramètres ya produit . | |||||
Eloko | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Komonana | Translucide . | ||||
Viscosité(pa.s) . |
2000 | 3000 | 4000 | 3500 | |
Bokasi ya makasi (Sorea) . | 30 | 40 | 50 |
40 |
|
Densité(g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Bokasi ya kokangama (MPA) . | 6.5 |
8.0 |
9.5 |
7.5 |
|
Elongation(%) . | 650 | 550 | 500 | 550 | |
Bokasi ya mayi ya miso (KN/M) . | 13 | 20 | 27 |
21 | |
linearshrinkage(%) . | 1.8 | 1.8 | 1.8 | 1.8 | |
CompressionSet 175 x 22h (%) . | - |
- |
- |
20 |