GA-2033
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A/B proportio 1 :1, 130°C x 5min x 15MPa
| Product parametri | |||||
| Productum | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
| Aspectus | Translucens | ||||
| Viscositas (Pa.s) |
2000 | 3000 | 4000 | 3500 | |
| Duritia (ShoreA) | 30 | 40 | 50 |
40 |
|
| Densitas (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
| Roboris distrahentes (MPa) | 6.5 |
8.0 |
9.5 |
7.5 |
|
| Prolongatio(%) | 650 | 550 | 500 | 550 | |
| Robur scindere (kN/m) | 13 | 20 | 27 |
21 | |
| Linearshrinkage(%) | 1.8 | 1.8 | 1.8 | 1.8 | |
| Compressionset 175 x 22H (%) | - |
- |
- |
20 |
|