GA-2033
Herchy
Framboð: | |
---|---|
Magn: | |
Próf: A/B hlutfall 1: 1, 130 ° C x 5min x 15mPa
Vörubreytur | |||||
Vara | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Frama | Hálfgagnsær | ||||
Seigja (pa.s) |
2000 | 3000 | 4000 | 3500 | |
Hörku (Shorea) | 30 | 40 | 50 |
40 |
|
Þéttleiki (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Togstyrkur (MPA) | 6.5 |
8.0 |
9.5 |
7.5 |
|
Lenging (%) | 650 | 550 | 500 | 550 | |
Társtyrkur (KN/M) | 13 | 20 | 27 |
21 | |
LinearShRinkage (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
Þjöppu 175 x 22H (%) | - |
- |
- |
20 |
Próf: A/B hlutfall 1: 1, 130 ° C x 5min x 15mPa
Vörubreytur | |||||
Vara | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Frama | Hálfgagnsær | ||||
Seigja (pa.s) |
2000 | 3000 | 4000 | 3500 | |
Hörku (Shorea) | 30 | 40 | 50 |
40 |
|
Þéttleiki (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Togstyrkur (MPA) | 6.5 |
8.0 |
9.5 |
7.5 |
|
Lenging (%) | 650 | 550 | 500 | 550 | |
Társtyrkur (KN/M) | 13 | 20 | 27 |
21 | |
LinearShRinkage (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
Þjöppu 175 x 22H (%) | - |
- |
- |
20 |