GA-2033
Herchy
| Eskuragarritasuna: | |
|---|---|
| Kopurua: | |
Proba: A/B erlazioa 1:1, 130°C x 5min x 15MPa
| Produktuaren parametroak | |||||
| Produktua | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
| Itxura | zeharrargitsuak | ||||
| Biskositatea (Pa.s) |
2000 | 3000 | 4000 | 3500 | |
| Gogortasuna (ShoreA) | 30 | 40 | 50 |
40 |
|
| Dentsitatea (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
| Trakzio erresistentzia (MPa) | 6.5 |
8.0 |
9.5 |
7.5 |
|
| Luzapena (%) | 650 | 550 | 500 | 550 | |
| Urraketaren indarra (kN/m) | 13 | 20 | 27 |
21 | |
| Uzkurdura lineala (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
| Konpresio multzoa 175 x 22H (%) | - |
- |
- |
20 |
|