GA-2033
Herchy
| Kasadiaan: | |
|---|---|
| Kuantitas: | |
Uji: Babandingan A/B 1:1, 130°C x 5min x 15MPa
| Parameter produk | |||||
| produk | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
| Penampilan | Tembus cahaya | ||||
| Viskositas (Pa.s) |
2000 | 3000 | 4000 | 3500 | |
| Teu karasa (ShoreA) | 30 | 40 | 50 |
40 |
|
| Kapadetan (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
| Kakuatan tegangan (MPa) | 6.5 |
8.0 |
9.5 |
7.5 |
|
| Elongation(%) | 650 | 550 | 500 | 550 | |
| Kakuatan cimata (kN/m) | 13 | 20 | 27 |
21 | |
| Linearshrinkage(%) | 1.8 | 1.8 | 1.8 | 1.8 | |
| Setrés komprési 175 x 22H (%) | - |
- |
- |
20 |
|