GA-2033
Gemetar
Ketersediaan: | |
---|---|
Kuantitas: | |
Tes: Rasio A/B 1: 1, 130 ° C x 5 menit x 15mpa
Parameter produk | |||||
Produk | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Penampilan | Tembus cahaya | ||||
Viskositas (Pa.s) |
2000 | 3000 | 4000 | 3500 | |
Kekerasan (Shorea) | 30 | 40 | 50 |
40 |
|
Kepadatan (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Kekuatan Tarik (MPA) | 6.5 |
8.0 |
9.5 |
7.5 |
|
Pemanjangan(%) | 650 | 550 | 500 | 550 | |
Kekuatan air mata (KN/m) | 13 | 20 | 27 |
21 | |
Linearshrinkage (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
Compressionset 175 x 22 jam (%) | - |
- |
- |
20 |
Tes: Rasio A/B 1: 1, 130 ° C x 5 menit x 15mpa
Parameter produk | |||||
Produk | GA-2033 |
GA-2043 | GA-2053 | GA-2045 | |
Penampilan | Tembus cahaya | ||||
Viskositas (Pa.s) |
2000 | 3000 | 4000 | 3500 | |
Kekerasan (Shorea) | 30 | 40 | 50 |
40 |
|
Kepadatan (g/cm3) | 1.10 | 1.12 | 1.14 | 1.13 | |
Kekuatan Tarik (MPA) | 6.5 |
8.0 |
9.5 |
7.5 |
|
Pemanjangan(%) | 650 | 550 | 500 | 550 | |
Kekuatan air mata (KN/m) | 13 | 20 | 27 |
21 | |
Linearshrinkage (%) | 1.8 | 1.8 | 1.8 | 1.8 | |
Compressionset 175 x 22 jam (%) | - |
- |
- |
20 |