Fluoroelastomer -FKM/FPM

Fluoroelastomer waa elastomer polymer synthetic oo ka kooban atamka fluorine ee atamka kaarboon ee silsiladda ugu weyn ama silsiladda dhinaca. Soo bandhigida atamka fluorine waxay siinaysaa caag kulayl aad u fiican, iska caabin oksaydh, caabbinta saliidda, caabbinta daxalka iyo iska caabinta gabowga atmospheric, waxaana si weyn loogu isticmaalaa hawada, duulista, baabuurta, batroolka iyo qalabka guriga.
Helitaanka:
Tirada:

Isku-dhafka caagga ah ee Fluoroelastomer-FKM


Alaabooyinka caagga ah ee FKM waxay leeyihiin iska caabin heerkul sare oo heer sare ah, iska caabin kiimiko ah, caabbinta saliidda, waxqabadka qallafsanaanta joogtada ah ee wanaagsan, caabbinta ololka iyo gaaska qulqulaya.


Fluoroelastomer waxaa inta badan loo adeegsadaa xiridda heerkul sare iyo mid hooseeya, qalabaynta vacuum iyo qalabka, qalabka kiimikada, baabuurta, duulista iyo meelaha kale.


Herchy Rubber waxay leedahay koox R&D ah oo xirfad leh si ay u daboolaan baahiyaha habaynta ee macaamiisheena.

●Nidaamka vulcanization Bisphenol iyo nidaamka vulcanization peroxide

● Samee oo soo saara alaabta wax lagu dhejiyo, duritaanka, extrusion iyo hababka kale ee farsamaynta.

● Ku beddel xarunta fluoroelastomer ee engegnaanta 50-90, midabyo iyo codsiyo kala duwan si waafaqsan shuruudaha macaamiisha.


Herchy Nooca Vulcanization Waxa ku jira fluorine Muunsanaanta Mooney Cufnaanta Xoog xajin Dheeraynta xilliga nasashada TR10 Dejinta cadaadiska Codsiga Dabeecad







200℃*72h ASTM D395 Nooca B
Darajo % ML (1+10)121℃ g/cm3 Mpa % ℃ %
FKM-65B20 Bisphenol 65.9 20 1.8 12.3 170 -17 17 O-rings; Gasket Dejinta cadaadiska hooseeya;
Dareeraha wanaagsan;
FKM-65B40 Bisphenol 65.9 40 1.81 14.3 180 -17 16 O-rings; Gasket Awood farsamo sare leh;
dejin cadaadis hooseeya
FKM-65B60 Bisphenol 65.9 60 1.81 15.5 180 -17 16 O-rings; Gasket Awood farsamo sare leh;
dejin cadaadis hooseeya
FKM-68B40 Bisphenol 68.5 40 1.85 14.3 220 -14 26 O-rings; Gasket Dareeraha wanaagsan;
Iska caabin heersare ah oo u adkaysta warbaahinta kiimikada;
Iska caabbinta heerkulka sare
FKM-68B60 Bisphenol 68.5 60 1.85 16.2 200 -14 26 O-rings; Gasket Xoog farsamo sare leh;
Iska caabin heersare ah oo u adkaysta warbaahinta kiimikada;
iska caabin heerkul sare ah
FKM-65B30S Bisphenol 65.9 30 1.80 15.0 190 -20 21 Badeecooyin dibadda ah, alaab la isku duray, alaab la qaabeeyey Iska caabbinta heerkulka hooseeya;
Awoodda farsamada sare;
dareere wanaagsan;
FKM-70P30 Peroxide 70 30 1.9 18.5 220 -7 36 Badeecooyin dibadda ah, alaab la isku duray, alaab la qaabeeyey Dareeraha wanaagsan;
caabbinta acid iyo alkaline heer sare ah;
Iska caabin heersare ah oo u adkaysta warbaahinta kiimikada;
Iska caabbinta heerkulka sare
FKM-68P45 Peroxide 68 45 1.85 16.5 280 -16 36 Badeecooyin dibadda ah, alaab la isku duray, alaab la qaabeeyey Dareeraha wanaagsan;
caabbinta acid iyo alkaline heer sare ah;
Iska caabin heersare ah oo u adkaysta warbaahinta kiimikada;
Iska caabbinta heerkulka sare


1.Shaabad

Shaabada mishiinka

Shaabadayda

Shaabada kiimikada

Shaabada uumiga oo aad u kulul

Makiinada shaambada Valve

Makiinada maqaarka

Saliidda saliidda


2. Hose

Tuubada caagga ah ee heerkulka sare

Tuubada shidaalka baabuurta

Tuubada shidaalka diyaaradaha

Dhuumaha wadajirka ah ee isku xiran


3. Fiilooyinka iyo fiilooyinka

Xadhkaha iyo fiilada ka samaysan fluoroelastomer ayaa si fiican u jilicsan oo waxay leedahay sifooyin dahsoon oo wanaagsan


4. Cajalada fiberglass ah

Heerkulka sare ee 300 ℃ iyo iska caabinta daxalka kiimikada


Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.