GA-2340
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: AB proportio ipsius 10:1 vel 1:1, 130' C x 5min x 15Mpa.
| Product parametri | |||
| Productum | GA-2340 |
GA-2341 | |
| Aspectus | Translucens | ||
| A/Bratio | A:B=10:1 |
A:B=1:1 |
|
| Viscositas (Pa.s) |
50/1 | 75/75 | |
| Duritia (ShoreA) | 38 | 38 | |
| Densitas (g/cm3) | 1.08 | 1.08 | |
| Roboris distrahentes (MPa) | 6.5 |
6.5 |
|
| Prolongatio(%) | 400 | 400 | |
| Robur scindere (kN/m) | 18 | 18 | |
| Linearshrinkage(%) | 2.0 |
2.0 | |