Applicatio: apta ad producendum casas calidas calcareas, caldarias stampas, calidum translatio cylindrum, exscriptorem cylindrum, etc.
Clavis lineamenta: excellentia resistentia ad caliditatem et humilem (60 'C -350 'C), altam mollitiam et bonam abrasionem resistentiae, humilis deformationes, difficile ad deformationem et fracturam, longam vitam servitutis.
Test: 1% curationis agentis (50% pasti DBPMH in gummi siliconis), 175' C x 5min x 15MPa.
| Product parametri | ||||||
| Productum | GA-5750 | GA-5770 | GA-5780 | GA-5741 | GA-5761 | |
| Aspectus | Canus | Fait flavo | ||||
| Duritia (ShoreA) | 55 | 70 | 80 | 43 | 60 | |
| Roboris distrahentes (MPa) | 5.5 | 6 | 7 | 6 | 8 | |
| Prolongatio(%) | 230 | 150 | 100 | 400 | 350 | |
| Robur scindere (kN/m) | 10 | 9 | 9 | 15 | 25 | |
| 175'C x22h Cogo(%) | 8 | 10 | 10 | 10 | 10 | |