GA-2340 ku vumba rhaba ya silicone ya mati yo engetela ya ku engetela (LSR) .

Ku tirhisiwa: Swi tirha eka ku humelerisa vutshila bya mavoko xivumbeko xa thermosetting resin, ku fana na, epoxy resin etc Swihlawulekisi swa nkoka: matimba ya le henhla, ku hatlisa ku horisa, dimensional stab小ty,tinomboro ta le henhla ta ku hundzuluka.
  • GA-2340

  • Herchy .

Ku kumeka:
Nhlayo: .

Xikambelo: Nhlayo ya AB ya 10:1 kumbe 1 :1, 130'C x 5min x 15Mpa.

Tipharamitha ta Xiendliwa .
Ximakiwa GA-2340
GA-2341
Xivumbeko Ku vonakala loku vonakaka
A/Bratio ya xirhendzevutani A:B=10:1
A:B=1:1
Viscosity(pa.s) .
50/1 75/75
Ku nonon'hwa (Shorea) . 38 38
Ku tsindziyela(g/cm3) . 1.08 1.08
Matimba ya ku tsana (MPA) . 6.5
6.5
Ku leha(%) . 400 400
Matimba ya ku handzuka (KN/M) . 18 18
linearshrinkage(%) . 2.0
2.0












Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.