GA-27X0 LSR pro Medical Qroducts (LSR)

Applicatio: varia genera sacculi, catheteri et alia producta medica
Clavis lineamenta: praeclara diaphaneitas et virtus alta, theauthenticatio 1S010993 biologicae testi compatibilitatis transi.
  • GA-2720

  • Herchy

Availability:
Quantity:

Test: A/B proportio 1 :1, 130°C x 5min x 15MPa


Product parametri
Productum GA-2720 GA-2730 GA-2740 GA-2750 GA-2760 GA-2770
Aspectus Perspicuus

Viscositas (Pa.s)
2000 3000 3000 3500
4000 5000
Duritia (ShoreA) 20 30 40 50
60
70
Densitas (g/cm3) 1.10 1.10 1.11 1.12 6.1.3
1.14
Roboris distrahentes (MPa) 7.0
8.0
9.5
10.0
10.0
9.5
Prolongatio(%) 880 800 700 550 500
350
Robur scindere (kN/m) 16 30 35
40 35
30
Linearshrinkage(%) 2.1 2.1 2.1 2.0 2.0
2.0








Priora: 
Next: 

ORIGINAL LINKS

Our Products

Contact Information

Add: No.33, Lane CLIX, Taiye via, Fengxian District, Shanghai
Tel / whatsapp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Flexilis Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.