GA-2340
Herchy
| Disponibilite: | |
|---|---|
| Kantite: | |
Tès: AB rapò 10:1 oswa 1:1, 130'C x 5min x 15Mpa.
| Paramèt pwodwi | |||
| Pwodwi | GA-2340 |
GA-2341 | |
| Aparans | Translusid | ||
| A/Bratio | A:B=10:1 |
A:B = 1:1 |
|
| Viskozite (Pa.s) |
50/1 | 75/75 | |
| Dite (ShoreA) | 38 | 38 | |
| Dansite (g/cm3) | 1.08 | 1.08 | |
| Fòs rupture (MPa) | 6.5 |
6.5 |
|
| elongasyon (%) | 400 | 400 | |
| Fòs chire (kN/m) | 18 | 18 | |
| lineyè kontraksyon (%) | 2.0 |
2.0 | |