GA-2340 ye
Herchy .
| A sɔrɔli: | |
|---|---|
| Hakɛ: . | |
Kɔrɔbɔli: AB hakɛ ye 10:1 walima 1 :1 ye, 130'C x 5min x 15Mpa.
| Product Paramɛtɛrɛw . | |||
| Ka kɛ | GA-2340 ye |
GA-2341 ye | |
| Yecogo | Translucent . | ||
| A/Bratio (Bratio) ye | A:B=10:1 ye |
A:B=1:1 ye |
|
| Viscosité(Pa.s) ka . |
50/1 ye | 75/75 kɔnɔ | |
| Gɛlɛya (Shoaa) . | 38 | 38 | |
| Densité(g/cm3) ye. | 1.08 | 1.08 | |
| Sɛgɛsɛgɛli fanga (MPa) . | 6.5 |
6.5 |
|
| Janya(%) . | 400 | 400 | |
| Ɲɛjibɔ fanga (KN/M) . | 18 | 18 | |
| Linearshrinkage(%) Bamako, Mali. | 2.0 |
2.0 | |