GA-2340 qoliplash qo'shimchasi bilan mustahkamlovchi suyuq silikon kauchuk (LSR)

Ilova: Epoksi qatroni va boshqalar kabi termoset qatronidan hunarmandchilik qoliplarini ishlab chiqarish uchun qo'llaniladi.
  • GA-2340

  • Herchi

Mavjudligi:
Miqdori:

Sinov: AB nisbati 10:1 yoki 1:1, 130'C x 5min x 15Mpa.

Mahsulot parametrlari
Mahsulot GA-2340
GA-2341
Tashqi ko'rinish Shaffof
A/Bratio A:B=10:1
A:B=1:1
Yopishqoqlik (Pa.s)
50/1 75/75
Qattiqlik (ShoreA) 38 38
Zichlik (g/sm3) 1.08 1.08
Kuchlanish kuchi (MPa) 6.5
6.5
Uzayish (%) 400 400
Yirilish kuchi (kN/m) 18 18
Chiziqli qisqarish (%) 2.0
2.0












Oldingi: 
Keyingisi: 

TEZKOR havolalar

MAHSULOTLARIMIZ

BOG'LANISH UCHUN MA'LUMOT

Qo'shish: №33, 159-tor ko'cha, Taiye yo'li, Fengxian tumani, Shanxay
Tel / WhatsApp / Skype: +86 15221953351
Mualliflik huquqi     2023 Shanghai Herchy Rubber Co., Ltd. Sayt xaritasi |   Maxfiylik siyosati | Qo'llab-quvvatlash Leadong.