GA-2340
Herchy
| Beskikbaarheid: | |
|---|---|
| Hoeveelheid: | |
Toets: AB-verhouding van 10:1 of 1:1, 130'C x 5min x 15Mpa.
| Produk parameters | |||
| Produk | GA-2340 |
GA-2341 | |
| Voorkoms | Deurskynend | ||
| A/Bratio | A:B=10:1 |
A:B=1:1 |
|
| Viskositeit (Pa.s) |
50/1 | 75/75 | |
| Hardheid (ShoreA) | 38 | 38 | |
| Digtheid (g/cm3) | 1.08 | 1.08 | |
| Treksterkte (MPa) | 6.5 |
6.5 |
|
| Verlenging (%) | 400 | 400 | |
| Skeursterkte (kN/m) | 18 | 18 | |
| Lineêre krimp (%) | 2.0 |
2.0 | |