GA-2340
Herchy
| kasedhiyan: | |
|---|---|
| Jumlah: | |
Tes: Rasio AB 10:1 utawa 1:1, 130'C x 5min x 15Mpa.
| Parameter produk | |||
| produk | GA-2340 |
GA-2341 | |
| Penampilan | Tembus | ||
| A/Bratio | A:B=10:1 |
A:B=1:1 |
|
| Viskositas (Pa) |
50/1 | 75/75 | |
| Kekerasan (ShoreA) | 38 | 38 | |
| Kapadhetan (g/cm3) | 1.08 | 1.08 | |
| Kekuatan tarik (MPa) | 6.5 |
6.5 |
|
| Elongasi (%) | 400 | 400 | |
| Kekuwatan sobek (kN/m) | 18 | 18 | |
| Linearshrinkage(%) | 2.0 |
2.0 | |