GA-26X0 Na-egosipụta nke ukwuu na ike dị elu LSR (LSR)

Ngwa: adabara maka imepụta ihe oriri kichin dị elu, ngwa igwu mmiri, ihe ụmụaka, wdg.
Njirimara ndị dị mkpa: ike dị elu, nghọta dị elu, ọkwa nri, gafere nkwenye nke RoHS, REACH, FDA na LFGB.
  • GA-2610

  • Herchy

Nnweta:
Ọnụọgụ:

Nnwale: Oke A/B nke 1:1, 130°C x 5min x 15MPa



Ngwa ngwaahịa


Ngwaahịa GA-2610 GA-2620 GA-2630 GA-2640 GA-2650 GA-2660 GA-2670 GA-2680
Ọdịdị N'ụzọ doro anya



Viscosity (Pa.s)
1500 2000 2500 3000 3500 4000
4000
5500
Isi ike (ShoreA) 10 20 30 40 50
60
70
80
Njupụta (g/cm3) 1.08 1.10 1.10 1.11 1.12
1.13
1.14
1.15
Ike tensile (MPa) 4.5
6.5
7.5
9.5
10.0
10.0
9.5
9.0
Mgbatị(%) 900 880 800 700 550
450
350
350
Ike akwa mmiri (kN/m) 8 12 15 25 35
35
30
30
Mbelata ahịrị (%) 2.3 2.1 2.1 2.1 2.0
2.0
2.0
2.0
Mbufe(%) 90
90 90 90 90 90 90 90




Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.