GA-91X3B
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
Kuedza: 1% yekurapa mumiririri (50% paste yeDBPMH mune silicone gum), 175 ° x5minx15MPa
| Product parameters | ||||
| Product | GA-9153B | GA-9163B | GA-9173B | GA-9183B |
| Chitarisiko | Nhema | |||
| Kuoma (ShoreA) |
50 |
60 |
70 |
80 |
| Density(g/cm3) | 1.16 |
1.18 |
1.21 |
1.22 |
| Tensile simba (MPa) |
9.0 |
8.0 |
7.0 |
7.0 |
| Elongation(%) | 500 |
400 |
300 |
150 |
| Simba rekubvarura (kN/m) | 20 |
20 |
16 |
16 |
| Kuramba kwepamusoro (Ω) | 105--106 | |||