GA-90×× Platinum Catalyzed Silicone Rubber yeExtrusion (HCR)

Chishandiso: chakakodzera kugadzira hose, rubber strip, kitchenware, nezvimwe. 
Akakosha maficha: kudzvanya uye extrusion molding, kujeka kwakanyanya uye yakanaka anti-yellowing pfuma, isiri-chepfu uye isingaravike, pfuura humbowo hweRoHS, REACH, FDA uye LFGB.
  • GA-9041

  • Herchy

Kuwanikwa:
Huwandu:

Muedzo: platinum vulcanizing agent, 130°C x 5min x 15MPa.

Product parameters
Product GA-9041
GA-9051 GA-9061 GA-9071 GA-9081
Chitarisiko Transparent
Williamplasticity
190
210
240
270
290
Kuoma (ShoreA)
40
50
60
70
80
Density(g/cm3) 1.13
1.16
1.18
1.19
1.21
Tensile simba (MPa)

9.0
10.0
10.0
9.5
9.0
Elongation(%) 900
700
600
500
400
Simba rekubvarura (kN/m) 30
35
35
35
35










Zvakapfuura: 
Zvinotevera: 

KUKURUMIDZA ZVINONYANYA

ZVINHU ZEDU

CONTACT INFORMATION

Wedzera: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Privacy Policy | Support By Leadong.