GA-9440 Silicone Rubber yeCable Accessories (Platinum) (HCR) ndeyepamusoro-inoshanda zvinhu zvakagadzirirwa kuda maapplication. Iyi platinamu-yakarapwa silicone rabha inopa kusimba kwakasimba uye kuramba kune yakanyanya kudzvanywa, ichiita kuti ive yakanakira akasiyana siyana matambo ekushandisa. Inopa yakanakisa kuvharwa kwemagetsi uye kuchinjika kwepamusoro, kuve nechokwadi chekushanda kwenguva refu kunyangwe mumamiriro akanyanya.
Iyi silicone rabha ine chitarisiko chinopenya uye inokodzera zvese zvemukati uye zvekunze application. Izvo zvinhu zvinogadzirwa kuti zvichengetedze kushanda kwepamusoro pasi pekushisa kwakanyanya uye kumanikidzwa, nepo simba rayo re dielectric uye kuramba kutevedza magetsi kunopa kuchengetedzwa kwakawedzerwa.
Iyo GA-9440 chigadzirwa inowanikwa mukuomarara kwakawanda uye kusimba kwesimba sarudzo, zvichiita kuti ive yakanyanya kurongeka kuzadzisa zvaunoda chaizvo. Kunyangwe iwe uri mumotokari, zvemagetsi, kana maindasitiri chikamu, iyi silicone rabha inovimbisa kuti tambo yako yemhando yepamusoro ndeyemhando yepamusoro.
Muedzo: kupora kweplatinum, A: 0.5%; B:0.7%; kutanga kurapa · 130°C x 10minutes, post kurapa: 200°C x 4H
| Product parameters | |
| Product | GA-9442 |
| Chitarisiko | Translucent |
| Williamplasticity |
160 |
| Kuoma (ShoreA) |
43 |
| Density(g/cm3) | 1.135 |
| Tensile simba (MPa) |
10.0 |
| Elongation(%) | 900 |
| Simba rekubvarura (kN/m) | 45 |
| Dielectric nguva dzose pa100HZ |
3.03 |
| Dissipation factor pa100HZ |
0.0029 |
| Tracking kuramba | -- |
| Dielectric Simba (kV/mm) | 23 |
| Kuramba Kwevhoriyamu (Ω·cm) | 1.0*1016 |

GA-9440 silicone rabha inopa yakakwira tensile simba uye kureba, ichipa yakawedzera kuita kwetambo accessories. Iyo inogadzirwa kuti imire kushushikana kwakanyanya uye kudzvanywa uku ichichengetedza chimiro chayo, ichiita kuti ive yakanakira kuvharira tambo uye cable accessories. Iyi yakakwirira-inoshanda silicone rubha inovimbwa nemakambani mazhinji epasi rose nekuda kwekuvimbika kwayo uye kuita zvakasiyana.
Iyi platinamu-yakarapwa silicone rabha inowanzoshandiswa mukutonhora shrink cable majoini uye 4G kutaurirana tambo. Kuchinjika kwayo uye yakakwira magetsi ekudzivirira zvivakwa inoita kuti ive yakakwana yekushandisa munharembozha uye magetsi emagetsi tambo. Isu tinopa GA-9440 kune akasiyana maindasitiri, anosanganisira emotokari, zvemagetsi, uye nharembozha, kuve nechokwadi chemhando yepamusoro mhinduro kune zvavanoda chaizvo.
GA-9440 silicone rabha inoita zvinonwisa mvura munzvimbo dzekupisa kwepamusoro, ichichengetedza kugadzikana uye kuvimbika kunyangwe pasi pemamiriro akanyanya. Iyi ficha inonyanya kubatsira kune yakakwirira-inoshanda tambo uye magetsi ekudzivirira zvinhu. Nekugadzikana kwayo kwakanyanya kupisa, chigadzirwa chedu chakagadzirirwa kusangana nezvinodiwa zvemaindasitiri emazuva ano.
Yedu silicone rabha inoenderana nezviyero zvepasi rese seRoHS uye REACH zvitupa. Inosangana nemirairo yezvakatipoteredza uye yekuchengetedza, kuve nechokwadi kuti zvinhu zvakachengeteka kuti zvishandiswe mumaindasitiri akaita senhare, mota, uye zvemagetsi. Isu tinoisa pamberi pemhando uye kuchengetedzeka kuendesa zvigadzirwa zvinoenderana nepasirese regulatory zviyero, zvichipa runyararo rwepfungwa kune vatengi vedu.
Isu tinopa tsika silicone rabha mhinduro, yakagadzirirwa kusangana nezvinodiwa zvekushandisa kwakasiyana, kungave kwetambo accessories kana magetsi ekudzivirira. Yedu GA-9440 chigadzirwa chinogona kugadziridzwa kune kwakasiyana kuomarara, kusimba kusimba, uye elongation zvinodiwa. Neanopfuura makore gumi echiitiko mumhinduro dzerubha, timu yedu inova nechokwadi chekukwana kwehunyanzvi hwako hwekuita.
GA-9440 silicone rabha inokunda pakupa yakakwira magetsi ekudzivirira. Izvi zvinoita kuti ive sarudzo yakanaka kwazvo yekushandisa mumatambo emagetsi, masisitimu emagetsi, uye mamwe maapplication anoda epamusoro ekudzivirira zvivakwa uye zviyero zvekuchengetedza. Chigadzirwa chedu chakakura chinotsigira kusikwa kwemhando yepamusoro, yakavimbika magetsi emagetsi kumisika yepasirese.
Kupokana kwerabha kune ozone uye mamiriro ekunze kunoita kuti ive chinhu chakanakira zvekunze tambo dzekushandisa uye telecom cable masisitimu. Inochengetedza kuvimbika kwayo uye kushanda nekufamba kwenguva, kunyangwe mumamiriro ezvinhu akaoma ezvakatipoteredza. Nekutarisa kwedu pakupa zvigadziriso zvenguva refu, GA-9440 inopa kuvimbika uye kuita kunoshingirira.
GA-9440 ine yakaderera shrinkage, iyo inobatsira kuchengetedza kushanda kwetambo accessories uye silicone rubber components nekufamba kwenguva. Ichi chivakwa chinonyanya kukosha munzvimbo dzakasimba uko kushoma deformation kunodiwa. Chikwata chedu kuHerchy chinoona kuti batch yega yega yeGA-9440 yakagadziridzwa kuita uye kusimba.
Q1: Ndeapi akakosha maapplication eGA-9440 silicone rubber ye cable accessories?
A1: GA-9440 yakanakira kuvharisa tambo, nharembozha, inotonhora shrink cable majoini, uye yakakwirira-inoshanda zvikamu zvemagetsi.
Q2: Ko GA-9440 silicone rabha inogona kugadzirwa kune chaiyo tambo yekuwedzera zvinodiwa?
A2: Hongu, isu tinopa zvigadziriso zvinogadziriswa kuti zvisangane nezvako zvehunyanzvi, kusanganisira kuoma uye kusimba kwesimba.
Q3: Ko GA-9440 silicone rabha inoita sei pasi pemamiriro ekunze ekupisa?
A3: GA-9440 inochengetedza kugadzikana uye kushanda mukupisa kwakanyanya, zvichiita kuti ive yakakodzera kune yakakwirira-tembiricha cable application.
Q4: Ko GA-9440 silicone rabha inoenderana nepasi rose kuchengetedza zviyero?
A4: Hongu, inosangana neRoHS, REACH, uye mamwe mazinga ekuchengetedza pasi rose, kuve nechokwadi chekushandiswa kwakachengeteka uye kwakavimbika mumaindasitiri akasiyana.
Q5: Ndeapi maindasitiri anoshandisa GA-9440 silicone rabha yetambo accessories?
A5: GA-9440 inoshandiswa zvakanyanya munharembozha, mota, masisitimu emagetsi, uye yakakwirira-inoshanda tambo kugadzira.
Q6: Ko GA-9440 silicone rabha inopa yakanakisa magetsi ekudzivirira zvivakwa?
A6: Hongu, inopa yakakwira dielectric simba, ichiita kuti ive yakakwana kune yemagetsi tambo yekuvharisa uye masisitimu emagetsi.
Q7: Ko GA-9440 silicone rabha kuramba kuchembera uye ozone kukuvara?
A7: Ehe, inopa kwakanakisa kuramba kuchembera, ozone, uye mamiriro ekunze, kuve nechokwadi chekugara kwenguva refu mumashandisirwo ekunze.
Q8: Ndingakumbira sei sampuli kana kuodha GA-9440 silicone rabha yepurojekiti yangu?
A8: Ingo taura nesu kune yetsika quote kana sampuli kuti uedze GA-9440 kune yako cable accessory application.