GA-91X0
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
Muedzo: 1% yekurapa mumiriri (50% paste yeDBPMH mune silicone gum), 175 ° x5minx15MPa
| Product parameters | |||||
| Product | GA-9130 |
GA-9140 | GA-9150 | GA-9160 | GA-9170 |
| Chitarisiko | Translucent | ||||
| Williamplasticity |
150 |
190 |
250 |
280 |
300 |
| Kuoma (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Density(g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.21 |
| Tensile simba (MPa) |
8.0 |
9.5 |
10.0 |
9.0 |
8.5 |
| Elongation(%) | 900 |
700 |
600 |
500 |
400 |
| Simba rekubvarura (kN/m) | 17 |
20 |
25 |
25 |
25 |
| Kuramba kwepamusoro (Ω) | 1011 |
||||