Neoprene, mtundu wa mphira wopangidwa ndi alpha-polymerization wa chloroprene, womwe umachokera ku 2-chloro-1,3-butadiene ngati chinthu chachikulu chopangira. Imatsutsanso ma acid ndi alkalis komanso ma reagents amankhwala. Imakhala ndi mphamvu zolimba kwambiri, kutalika kwake, komanso kusinthika kosinthika, kumamatira kwabwino. Kukalamba ndi kukana kutentha. Zabwino kwambiri pakukana kwamafuta komanso kuwonongeka kwamankhwala. Kukana kwanyengo ndi kukana kukalamba kwa ozone ndi rabara ya ethylene propylene ndi mphira wa butyl pambuyo pake. Kukana kutentha ndi kofanana ndi NBR, ndi kutentha kwa 230-260 ℃; kukana kwakanthawi kochepa ndi 120-150 ℃, komwe kumagwiritsidwa ntchito kwa nthawi yayitali pa 80-100 ℃, komwe kulinso ndi zinthu zina zoletsa moto. Kukana kwa dzimbiri kwa inorganic acid ndi alkalis. Herchy Rubber yotengera chidziwitso chochuluka muukadaulo wa raba komanso njira zambiri zogawa mawu. Amatumizidwa ku mayiko oposa 15 USA, Russia, Brazil, Argentina, Korea, Germany, Italy, Spain, Australia, India, etc.Neoprene, mphira kupanga opangidwa ndi alpha-polymerization wa chloroprene (ie, 2-chloro-1,3-butadiene) monga yaikulu yaiwisi.Ili ndi katundu wabwino thupi ndi makina, kukana mafuta alzokali, kukana mafuta alzokali ndi kukana kutentha kwa dzuwa, kukana kwa mafuta a ozokali ndi kutentha kwa dzuwa, kukana kwa mafuta ndi kutentha kwa dzuwa kukana reagent.
Ali ndi mphamvu zamakokedwe apamwamba, elongation ndi crystallinity yosinthika, kumamatira kwabwino. Kugonjetsedwa ndi ukalamba ndi kutentha. Kukana kwabwino kwa mafuta ndi dzimbiri lamankhwala. Kukana kwanyengo ndi kukana kukalamba kwa ozone ndi chachiwiri kwa mphira wa ethylene propylene ndi mphira wa butyl. Kutentha kwa kutentha kumafanana ndi NBR, kutentha kwa kutentha kwa 230-260 ℃, kukana kwakanthawi kochepa 120-150 ℃, kugwiritsidwa ntchito kwa nthawi yayitali pa 80-100 ℃, ndi digiri inayake yamoto wamoto. Kukana kwa dzimbiri kwa inorganic acid ndi alkalis.
Herchy Rubber kutengera chidziwitso chochuluka muukadaulo wa raba komanso njira zambiri zogawa mawu, zotumizidwa kumayiko opitilira 15 monga USA, Russia, Brazil, Argentina, Korea, Germany, Italy, Spain, Australia, ndi India etc.
| Herchy | Zosintha | Crystallinity | Kukhuthala kwa Mooney | Dupont | Denka | Lanxess | Kugwiritsa ntchito |
| Gulu | ML(1+4)100℃ | Neoprene | Baypren | ||||
| Mtengo wa CR1211 | Sulfure | Pang'onopang'ono | 30-45 | GNA | PM-40 | 711 | Malamba otengera mgodi, malamba otumizira magetsi, mapaipi, zosindikizira, mawaya ndi ma jekete a chingwe |
| Mtengo wa CR1212 | Sulfure | Pang'onopang'ono | 46-60 | GNA | PM-40 | 711 | Malamba otengera mgodi, malamba otumizira magetsi, mapaipi, zosindikizira, mawaya ndi ma jekete a chingwe |
| Mtengo wa CR2321 | Xanthates / Mercaptan | Wapakati | 35-45 | WM1 | M30/M40 | 211 | Mipiringidzo yowonjezera, ma hose, matepi, zisindikizo za rabala, mawaya ndi ma jekete a chingwe |
| Mtengo wa CR2322 | Xanthates / Mercaptan | Wapakati | 46-55 | W | M40/M100/M120 | 210 | Mipiringidzo yowonjezera, ma hose, matepi, zisindikizo za rabala, mawaya ndi ma jekete a chingwe |
| Mtengo wa CR3221 | Zosakaniza-zosintha | Wapakati | 30-45 | GW | Chithunzi cha DCR-40 | 510 | Malamba otumizira mgodi, malamba otumizira magetsi, mapaipi, zosindikizira, ma cushion, mawaya ndi ma jekete a chingwe. |
| Mtengo wa CR3222 | Zosakaniza-zosintha | Wapakati | 46-60 | GW | Chithunzi cha DCR-40 | 610 | Malamba otumizira mgodi, malamba otumizira magetsi, mapaipi, zosindikizira, ma cushion, mawaya ndi ma jekete a chingwe. |
| Mtengo wa CR2441 | Xanthates / Mercaptan | Mofulumira | 25-34* | AD-10 | A-70 | 310 | Zomatira |
| Mtengo wa CR2442 | Xanthates / Mercaptan | Mofulumira | 35-53* | AD-20 | A-90 | 320 | Zomatira |
| Mtengo wa CR2443 | Xanthates / Mercaptan | Mofulumira | 54-75* | AD-30 | A-100 | 330 | Zomatira ndi tack yapamwamba. |
| Mtengo wa CR2444 | Xanthates / Mercaptan | Mofulumira | 76-115* | AD-40 | A-120 | 340 | Zomatira ndi tack yapamwamba. |
| Mtengo wa CR244A | Xanthates / Mercaptan | Mofulumira | 116-140* | AD-40 | A-400 | 340 | Kusintha mamasukidwe akayendedwe, kusintha koyamba adhesion |
| Mtengo wa CR244B | Xanthates / Mercaptan | Mofulumira | pamwamba 140 * | AD-40 | A-400 | 340 | Kusintha mamasukidwe akayendedwe, kusintha koyamba adhesion |
| Mtengo wa CR248 | Xanthates / Mercaptan | Mofulumira | ADG | A-90S | 320P | Zomatira | |
| Chithunzi cha DCR1141 | Sulfure | Pang'onopang'ono | 30-45 | Mtengo wa GRT | PS-40 | Ndi bwino kutentha kutsika resistance.Mipiringidzo Extruded, hose, matepi, mphira zisindikizo, waya ndi ma jekete chingwe | |
| Chithunzi cha DCR1142 | Sulfure | Pang'onopang'ono | 46-60 | Mtengo wa GRT | PS-40 | Ndi bwino kutentha kutsika resistance.Mipiringidzo Extruded, hose, matepi, mphira zisindikizo, waya ndi ma jekete chingwe | |
| Chithunzi cha DCR2131 | Xanthates | Pang'onopang'ono | 35-45 | WRTM1 | S-40V | 116 | Ndi bwino kukana kutentha kwapansi. Malamba otengera mgodi, malamba otumizira magetsi, mapaipi, zosindikizira, mawaya ndi ma jekete a chingwe |
| Chithunzi cha DCR2132 | Xanthates | Pang'onopang'ono | 46-55 | WRT | Chithunzi cha DCR-66 | 126 | Ndi bwino kukana kutentha kwapansi. Malamba otengera mgodi, malamba otumizira magetsi, mapaipi, zosindikizira, mawaya ndi ma jekete a chingwe |
*Kukhuthala kwa Brinell kwa 5% toluene solution
1. Hoses
Ma hoses a kuthamanga kwambiri komanso kuthamanga kwambiri, kuthamanga kwapakatikati komanso kutsika
Mafuta ophikira ndi mafuta ophikira
Ananyema payipi
Ma hoses omwe amagwiritsidwa ntchito m'mafakitale a petroleum
2. Zingwe ndi mawaya
Zingwe zoyanika za mphira
Zingwe zotsatsira
Zingwe zowotcherera
Lathyathyathya flexible mphamvu ndi zingwe zowongolera
Zingwe zoyatsira zathyathyathya
3. Malamba otumizira ndi kutumiza
Malamba otumizira ufa wamagalimoto ndi makampani onse
Malamba nthawi
Malamba a Poly-V
Malamba a V-lamba
Malamba ovala jekete a V
Malamba otumizira okhala ndi zingwe zachitsulo ndi zolimbikitsira zovala zamafakitale
4. Zigawo zoumbidwa
Mavuvu ndi fumbi zipewa
nsapato za Axle
Zigongono
Zisindikizo
Zinthu za masika
Dampers ndi ma bearings
Mitundu ya Windshield wiper
5. Zisindikizo zosindikizira
Mizere yosindikizira yolimba komanso ya microcellular
Zowonjezera zosindikizira zamagulu
6. Fomu
Pepala la mphira wa thovu la suti zonyowa
Zingwe za Corthopedic