GA-57XX
Herchy
| kupezeka: | |
|---|---|
| kuchuluka: | |
Kugwiritsa ntchito: koyenera kupanga machira otentha, masitampu otentha, chogudubuza chotentha, chodzigudubuza, etc.
Zofunika kwambiri: kukana kwambiri kutentha kwambiri ndi kutsika (60 'C -350 'C), kulimba mtima kwakukulu ndi kukana kwabwino kwa abrasion, kutsika kwapang'onopang'ono, zovuta kupindika ndi kusweka, moyo wautali wautumiki.
Kuyesa: 1% ya machiritso (50% phala la DBPMH mu chingamu cha silikoni), 175'C x 5min x 15MPa.
| Zogulitsa katundu | ||||||
| Zogulitsa | GA-5750 | GA-5770 | GA-5780 | Mtengo wa GA-5741 | Mtengo wa GA-5761 | |
| Maonekedwe | Hoary | Fait yellow | ||||
| Kuuma (ShoreA) | 55 | 70 | 80 | 43 | 60 | |
| Mphamvu yamagetsi (MPa) | 5.5 | 6 | 7 | 6 | 8 | |
| Kutalikira (%) | 230 | 150 | 100 | 400 | 350 | |
| Mphamvu yamisozi (kN/m) | 10 | 9 | 9 | 15 | 25 | |
| 175'C x22h Kuponderezedwa (%) | 8 | 10 | 10 | 10 | 10 | |