GA-97XX Oil Resistant Silicone Rubber (HCR)

GA-97XX Oil Resistant Silicone Rubber (HCR)
Kugwiritsa ntchito: koyenera kupanga zinthu zosagwirizana ndi mafuta.
Zofunika kwambiri: kulimba kwambiri, kulolerana bwino ndi ASTM 1# ndi Mafuta a IRM903, perekani kutsimikizika kwa RoHS ndi REACH.
 
  • GA-97XX

  • Herchy

kupezeka:
Kuchuluka:

GA-97XX Oil Resistant Silicone Rubber (HCR)


Kugwiritsa ntchito: koyenera kupanga zinthu zosagwirizana ndi mafuta.
Zofunika kwambiri: kulimba kwambiri, kulolerana bwino ndi ASTM 1# ndi Mafuta a IRM903, perekani kutsimikizika kwa RoHS ndi REACH.
Mayeso: 1% ya mankhwala ochiritsira (50% phala la DBPMH mu chingamu cha silicone), 175 ° Cx5min x15MPa.



Zogulitsa katundu
Zogulitsa GA-9740 GA-9750 GA-9760 GA-9770
Maonekedwe Imvi
Williamplasticity 140 180 200 260
Kuuma (ShoreA) 40 50 60 70
Kachulukidwe (g/cm3) 1.23 1.25 1.28 1.32
Mphamvu yamagetsi (MPa) 3.5 4.5 5 5.5
Kutalikira (%) 700 600 400 250
Mphamvu yamisozi (kN/m) 15 15 15 15
175'C x22h Kuponderezedwa (%) 20 20 20 20
Kukalamba kwa mpweya 225°C x70H Kusintha kwamphamvu 1 2 2 2
Kusintha kwamphamvu kwamphamvu -25% -25% -25% -25%
Kusintha kwa elongation -30% -30% -30% -30%
IRM903mafuta 150°C x70H Kusintha kwamphamvu -18 -18 -17 -16
Kusintha kwamphamvu kwamphamvu -35% -35% -35% -35%
Kusintha kwa elongation -20% -20% -20% -20%
Kusintha kwa mawu 36% 36% 35% 35%


Zam'mbuyo: 
Ena: 

MALANGIZO OPHUNZITSA

ZOPHUNZITSA ZATHU

ZAMBIRI ZAMALUMIKIZIDWE

Onjezani: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Ufulu     2023 Shanghai Herchy Rubber Co., Ltd. Mapu atsamba |   Mfundo Zazinsinsi | Support By Leadong.