GA-57XX ya go swana le yona
Herchy .
| Go hwetšagala: | |
|---|---|
| Palo: . | |
Kopo: loketseng bakeng sa hlahisa chesang setempe cots, chesang setempe poleiti, chesang phetiso rolara, copier rolara, joalo-joalo.
litšobotsi tse senotlolo: babatsehang ho hanyetsa ho phahameng le tlaase mocheso (60 'C -350 'C), phahameng manyela le molemo abrasion ho hanyetsa,tlaase deformation sete, thata ho deformationand robeha, nako e telele tšebeletso bophelo.
Teko: 1% ya moemedi wa go fodiša (50% ya peista ya DBPMH ka gare ga mare a silicone),175'C x 5min x 15MPa.
| Ditekanyetšo tša Setšweletšwa . | ||||||
| Setšweletšwa | GA-5750 ya go swana le yona | GA-5770 ya go swana le yona | GA-5780 ya go swana le yona | GA - 5741 ya go swana le | GA-5761 ya go swana le | |
| Ponagalo | Hoary ya go swana | Fait mosehla | ||||
| Go thatafala (Sorea) . | 55 | 70 | 80 | 43 | 60 | |
| Matla a go goga (MPA) . | 5.5 | 6 | 7 | 6 | 8 | |
| go telefa (%) . | 230 | 150 | 100 | 400 | 350 | |
| Matla a Meokgo (KN/M) . | 10 | 9 | 9 | 15 | 25 | |
| 175 'C x22h Kgatelelo (%) . | 8 | 10 | 10 | 10 | 10 | |