O mo: Gae » Ditšweletšwa » Rabara ya tswako . » Silicone ya VMQ » GA-200X Ga go na Rabara ya Silicone ya Seela ya go fodiša ka morago ga go fodiša (LSR)

Go Laetša .

Abelana go: .
Konopo ya go abelana ya Facebook .
Konopo ya go abelana ya Twitter .
Konopo ya go abelana ka mola .
WeChat go abelana konope .
Konopo ya go abelana ya LinkedIn .
Pinterest Konopo ya go abelana .
WhatsApp go abelana konope .
AbelanaThis konopo ya go abelana .

GA-200X Ga go na rabara ya silicone ya seela ya ka morago ga go fodiša (LSR) .

Kopo: loketseng bakeng sa hlahisa masea sehlahiswa, tse kang, lesea letswele, lesea botlolo,bj.bj.
Key litšobotsi: tlaase feto-fetoga le maemo taba, phahameng pepeneneng, babatsehang mochine thepa,feta netefatso ea RoHS, REACH, FDA, le LFGB
  • GA - 2002 ya go swana le

  • Herchy .

Availability:
Palo:

Teko: A / B karo-karolelano ya 1 :1, 130 ° C x 5min x 15MPa


Ditekanyetšo tša Setšweletšwa .
Setšweletšwa GA - 2002 ya go swana le GA - 2003 ya go swana le GA - 2004 ya go tšhungwa GA - 2005 GA - 2006 ya go swana le GA - 2007
Ponagalo Pepeneneng

Go thatafala (Sorea) . 23 30 40 50
62
68
Kitlano (G / CM3) . 1.10 1.12 1.12 1.13 1.14
1.14
Matla a go goga (MPA) . 6.0
8.0
9.0
9.0
10.0
9.5
go telefa (%) . 750 650 600 500 450
400
Matla a Meokgo (KN/M) . 10 15 20
25 30
35
Diteng tša VOC(%) . 0.35 0.35 0.3 0.3 0.3 0.3







Peleng: 
Latelago: 

Dikgokagano tša ka pela .

Ditšweletšwa tša rena .

TSHEDIMOŠO YA KGOKAGANO

Add: No.33, Lane 159, Tsela ya Taiye, Setereke sa Fengxian, Shanghai
Mogala / WhatsApp / Skype: +86 15221953351
E-mail: .  info@herchyrubber.com
Tokelo ya ngwalollo e ileditšwe     2023 Shanghai Herchy Rabara Co., Ltd. Mmapa wa Sebaka |   Pholisi ya Sephiri | Thekgo Ka Leadong ..