Dithoto:
Kganetšo ya themperetšha ye e feteletšego (-20°C go ya go +250°C).
Kganetšo ye e kgethegilego ya oli, dibešwa, disolvent, diesiti, le metheo.
Matla a go goga a godimo (10-20 MPa), sete ya kgatelelo ya fase (<15% ka 150°C/70h).
Kgabo retardant (UL94 V-0 tekanyetso) le ozone-thibela.
Mehola: .
E hlakantšwe pele le dihlare tša go fodiša (mohlala, bisphenol AF, peroxide) bakeng sa vulcanization ye e šomago gabotse.
E boloka go tsepama ga dimenšene ka ditikologong tša dikhemikhale tše bogale.
Mephato yeo e obamelago FDA yeo e hwetšagalago bakeng sa go ikgokaganya le dijo/ka tša kalafo.
Ditirišo: .
Sefofane: Di-O-ring tša tshepedišo ya makhura, ditiiso tša entšene le di- diaphragm.
Koloi: Di-gasket tša turbocharger, ditiiso tša phetišetšo le di- injector tša makhura.
Dikhemikhale: Di- lining tša pompo, ditulo tša di-valve le dikopano tša dihose.
Dithoto:
Kganetšo ya phišo go fihla go +150°C (go kgaotša +175°C).
Go ganetša mo go phagamego ga oli, di- amine le diela tša haeteroliki.
Phahameng tensile matla (15-35 MPa) le mokhathala ho hanyetsa.
Go tsenelela ga fase go dikgase.
Mehola: .
Pre-vulcanized bakeng sa fokotswa tshebetso nako.
E boloka elasticity ka tlase ga go pepentšhwa ka nako e telele go methopo ya ditaba e thata.
E hwetšagala ka mephato yeo e fodišitšwego ka peroxide goba sebabole.
Ditirišo: .
Oli & Gase: Diphuthelwana tša go phunya, ditiiso tša pompo ya leraga, le dikarolo tša hlogo ya sediba.
Koloi: Mabanta a nako, ditshepedišo tša go tsenya makhura le dihose tša turbocharger.
Industrial: Ditiiso tša silindara ya haeteroliki le dikarolo tša gearbox.
Dithoto:
Kganetšo ya oli ye e lekanetšego (e kaone go feta EPDM, ka fase ga HNBR).
Thempheretšha ya go fapana: -40°C go ya go +120°C.
Phahameng abrasion ho hanyetsa (ASTM D5963: 100-200 mm3 tahlehelo).
Good resilience le compression beha ho hanyetsa.
Mehola: .
Ditshenyagalelo-atlehang le moldability babatsehang.
Customizable acrylonitrile dikahare (18-50%) bakeng sa tailored oli ho hanyetsa.
Ditirišo: .
Koloi: Dihose tša makhura, di-O-ring le ditiiso tša phetišetšo.
Diintaseteri: Mabanta a go sepetša, di-roller tša go gatiša le ditiiso tša haeteroliki.
Moreki: Diatlana tša latex le didirišwa tša dipapadi.
Dithoto:
Kganetšo ye e tšwetšego pele ya ozone / boemo bja leratadima (diiri tše 5,000+ ka diteko tša QUV).
Thempheretšha ya go fapana: -50°C go ya go +150°C.
Matla a phahameng a dielectric (20-30 kV / mm) le metsi impermeability.
Tlaase khase permeability.
Mehola: .
Pre-formulated le antioxidants le UV stabilizers.
E babatsehang thothometsa damping (tahlehelo Ntlha: 0.1-0.3).
Ditirišo: .
Koloi: Ditiiso tša mojako, dihose tša radiator le di- mount tša entšene.
Kago: Dimembrane tša go rulela, di- liner tša letamo le di- gasket tša mafasetere.
Motlakase: Cable kwahelang le matla phetiso mabanta.
Dithoto:
Matla a godimo a go goga (20-60 MPa) le elasticity (go fihla go 800% elongation).
Ikhethang abrasion ho hanyetsa (ASTM D5963: 20-50 mm3 tahlehelo).
Thempheretšha ya go fapana: -40°C go ya go +100°C (go fihla go +120°C ka di-stabilizer tša phišo).
E hanyetsa solvents le hydrolysis.
Mehola: .
Go thatafala mo go ka fetošwago (Shore A 50-95).
E hwetšagala ka mephato ya go tšhollwa, ya go šilwa goba ya polasetiki ya go fiša.
Ditirišo: .
Intasteri: Maotwana, di-roller le mapanta a go sepetša.
Dikoloi: Dibushing tša go emiša, di-shock absorber le dibutšwana tša go kopanya CV.
Bongaka: Di- catheter, di- brace tša marapo le dilo tša maitirelo.
Dithoto:
Kganetšo ya phišo ye e tšwelago pele go fihla go +150°C (go kgaotša +175°C).
Kganetšo e botse kudu go diela tša phetišetšo ya go itiriša (ATF), dioli le phišo.
Ozone e lekanetšego le go ganetša boemo bja leratadima.
Matla a go goga: 7-15 MPa.
Mehola: .
E hlakantšwe pele le di-curative tša amine goba peroxide bakeng sa go fodiša ka lebelo.
E boloka go tsepama ga dimenšene ka ditikologong tša ATF.
Ditirišo: .
Koloi: Ditiiso tša phetišetšo, di-O-ring le di- diaphragm tša pompo.
Matla go laola tsamaiso dikarolo.
Intasteri: Ditiiso tša pompo tša methopo ya ditaba ye e theilwego godimo ga oli.
Dithoto:
Wide thempereichara fapaneng (-40 ° C ho + 150 ° C).
Go ganetša oli, di- glycol le go fetoga ga boemo bja leratadima.
Phahameng tensile matla (10-20 MPa) le compression beha ho hanyetsa.
Go tsenelela ga fase go dikgase.
Mehola: .
E lekalekanya go ganetša phišo le go fetofetoga le maemo.
E lwantšha hydrolysis le botšofadi.
E hwetšagala ka mephato yeo e fodišitšwego ka peroxide goba sebabole.
Ditirišo: .
Koloi: Dihose tša radiator, dikarolo tša tshepedišo ya setšidifatši le dihose tša go tsenya moya.
Intasteri: Mabanta a go sepetša bakeng sa go swara dikhemikhale le di-diaphragm tša pompo.
HVAC: Di-gasket tša diphaephe le di-isolator tša go thothomela.