Tunlai thil siamnaah hian synthetic rubber hi a pawimawh hle. Kum 2023 khan khawvela rubber hman zawng zawng zinga 58% vel a ni. Synthetic rubber chi hrang hrang hman tlanglawn ber chu:
Styrene-Butadiene Rubber (SBR) hmanga siam a ni.
Polybutadiene Rubber (BR) hmanga siam a ni.
Ethylene-Propylene-Diene Monomer (EPDM) hmanga siam chhuah a ni.
Isobutylene-Isoprene Rubber (IIR) hmanga siam a ni.
Polyisoprene Rubber (IR) hmanga siam a ni.
Nitrile Rubber (NBR) hmanga siam a ni.
Chloroprene Rubber (CR) hmanga siam a ni.
Acrylic Rubber (ACM) hmanga siam a ni.
Hydrogenated Nitrile Rubber (HNBR) hmanga siam chhuah a ni.
Synthetic rubber hi elastomer an ti bawk. Mihring siam an ni a, thilsiamah hmuh tur an awm lo. Heng elastomer te hi natural rubber aiin an chak zawk a, an daih rei zawk fo bawk. Industry tam takah an hmang a, car siam leh siamnaah te pawh an hmang nasa hle. Rubber chi hrang hrang hriat hian engineer leh hnathawkte chu hna tin atan a dik ber thlan nan a pui thin. A hnuaia table-ah hian tun hnaia khawvel hmun hrang hranga synthetic rubber hralh chhuah zat tarlan a ni:
| Kum | Global Synthetic Rubber Market Size (USD Billion) |
|---|---|
| 2023 | ~41.04 a ni |
| 2024 | 38.90 |
| 2025 | 41.04 (projected) a ni ang. |
| 2034 | 66.44 (hmasawnna) . |
Synthetic rubber hi mihring siam a ni. Tire, seal, hose, leh thil dang tam takah hman a ni. Natural rubber aiin a rei zawk. Hna hrang hrang nena inmil turin thlak theih a ni bawk.
An awm synthetic rubber chi hrang hrang . Type tin hian chakna bik an nei vek a. SBR hi tyre tan a tha. NBR hian oil nen a thawk tha hle. Khua chhe tan chuan EPDM hi a tha ber. Silicone hi lumna atan leh damdawi atan hman a ni.
Hna tin atan synthetic rubber dik tak i thlan a ngai a ni. Temperature, chemical, a bendy zia leh a senso ang chi te hi ngaihtuah teh.
Santoprene ang chi synthetic rubber tam tak chu hman leh theih a ni. Hei hian bawlhhlawh tihtlem nan a pui a, lei pawh a tifai zawk bawk.
Rubber tin hian eng nge an tih theih tih hriat hian engineer leh siamtute a pui hle. A tha ber an thlang thei. Hei hian thil siamte a tichak a, a him zawk a, rei zawk a daih bawk.
Synthetic rubber hi mihring siam a ni a, nature-ah hmuh tur a awm lo. Natural rubber angin a thawk nasa hle. Heng thilte hi elastomer an ti a, a chhan chu an inzawm khawm thei a, an pianziaah an kir leh thei a ni. Factory-te chuan oil atanga chemical hmangin elastomer an siam thin. Synthetic rubber hi natural rubber ang deuh a ni a, mahse hna bik atan chuan thlak theih a ni.
Note: Synthetic rubber chi hrang hrang a awm a, chu chu styrene-butadiene rubber, butyl rubber, leh silicone rubber te hi a ni. A chi tin hi a kawng hrang hrangah a chak a, thil chi hrang hrang atan hman a ni.
Chemical industry chuan synthetic rubber hi elastomer eng pawh vulcanized theih a ni a, chemicals inzawmkhawma siam a ni an ti. He pawl hian acrylate rubber, butadiene-styrene copolymer, nitrile-butadiene rubber leh a dangte an nei a. Heng elastomer te hi tyre, seal, hose leh thil dang tam tak siamna atan a pawimawh hle.
Synthetic rubber siam hi oil hmanga siam thil hmanga tan a ni. Factory-ah chuan naphtha ang chi thil an hmang a, chu chuan natural gas nen an inrem a, monomers an siam thin. Monomer te hi thil butadiene, styrene, isoprene, chloroprene, acrylonitrile, . ethylene , leh propylene te a awm bawk. Polymerization chu monomers inzawmkhawma chain sei tak tak polymer an tih siamna a ni.
Elastomer tam zawk hian carbon atom atanga siam backbone an nei a, mahse silicone rubber hian silicon leh oxygen atanga siam backbone a nei thung.
Silicone rubber hi silicon atanga lo chhuak a ni a, chu chu sand emaw quartz emaw ah a awm a ni.
Catalyst hrang hrang leh monomer mix te hian elastomer te a chhuah dan tur control nan a pui thin. Polymerization hnuah chuan material chu vulcanization kaltlangin a kal a. He step hian sulfur ang chi thil hmangin rubber chu a khauh leh chak zawk a siam a ni. Chemical structure thlak danglam hian factory te chu special use tam tak atan elastomers an siam thei a ni.
Styrene-butadiene rubber hi khawvel hmun hrang hrangah an hmang nasa hle. Factory-te chuan butadiene tam zawk leh styrene engemaw zat an pawlh hmangin an siam thin. He mix hian material chak tak leh bendy tak a siam a ni. SBR hi a chhe awlsam lo va, metal-ah a innghat tha hle. Hmun lum leh lum takah a thawk a, -60oF atanga +225oF thleng a thawk thei. SBR hi tyre siam nan an hmang tam ber a, SBR siam tam zawk hi an hmang a ni. Belt, hose, wire, pheikhawk kephah, leh ei tur bungruaah te pawh a awm bawk. SBR hi a man a to lo va, hna tam takah a thawk tha hle. Mite chuan tyre siam that nan SBR hi natural rubber nen an pawlh fo thin.
Note: SBR hi natural rubber nena chawhpawlh a ni a, hei hian tires a rei zawk theih nan a pui a ni.
Butadiene rubber hi synthetic rubber chi pawimawh dang a ni bawk. Bouncy tak a ni a, a stretch nasa thei bawk. BR hi a tear awlsam lo va, rei tak a daih. Khua lum leh vawt ah pawh a thawk tha hle. BR hi tyre, gasket, seal, leh pheikhawk sole-ah te hman a ni. Conveyor belt, sports gear, leh damdawi hmanruaah te pawh a awm bawk.
Nitrile rubber hi Buna-N an ti bawk. Acrylonitrile leh butadiene atanga siam a ni. NBR hian oil, fuel, leh chemicals te a do thiam hle. Car leh thlawhna chhunga seal, gasket leh hose siamna atan hman a ni. NBR hi oil leh gas hmanrua leh medical gloves-ah te pawh hman a ni. Engine leh fuel system-ah a thawk tha hle a, a chhan chu oil-ah a chhe lo. NBR hi a chak a, hmun harsaah pawh rei tak a daih.
EPDM hi synthetic rubber a ni a, ni, ruah leh ozone lakah pawh a ding thei a ni. Khua lum leh vawt ah pawh bendy takin a awm reng. EPDM hi tui emaw chemical tam takin a tichhia lo. A man tlawm a, recycle theih a ni. EPDM hi car kawngkhar, hose, inchung, leh air system-ah te hman a ni. Pawn lam emaw, khaw lum lai emawa hman tur thil atan duhthlanna tha tak a ni.
Neoprene hi chloroprene rubber an ti bawk. A khauh a, a bendy a, oil hian a tichhe lo. Neoprene hian stress leh temperature inthlak danglamna a tuar thei a ni. Car-ah gasket, hose, leh mount atan hman a ni. Building-ah chuan seal leh pad atan an hmang thin. Neoprene hi wetsuit, safety gear, leh belt-ah te pawh a awm a, a chhan chu khaw lum leh chemical a do thei a ni.
Butyl rubber hian gas chu awlsam takin a paltlang tir lo. Hei hian tire tube leh damdawi bottle cap atan a tha hle. A bendy reng a, tire chhungah boruak a vawng reng bawk. Butyl rubber hian damdawi tui leh chemical lakah a veng bawk. Thil mamawh bikte nena inmil turin thlak theih a ni a, damdawi seal-te tan a dam thuai theih ang.
Chlorinated polyethylene hi synthetic rubber chak leh flexible tak a ni. Khua lum, hriak, mei leh khaw lum leh khaw vawt lakah a ding thei a ni. CPE hi wire cover, hose, leh car part hrang hrang atan hman a ni. Mix leh shape a awlsam hle. CPE hian temperature tam takah hna a thawk tha a, awlsam takin kangmei a chhuah lo.
Acrylic rubber hi car-ah an hmang nasa hle. Heat sang tak, oil a la thei a, a upa nghal vat lo. ACM hi seal, hose, gasket, leh glue-ah te hmuh tur a awm. Noise tihtlem nan a pui a, car parts te pawh a rei zawk bawk. ACM hi fuel system parts atan pawh a tha a, car kawngkhar atan glue a hmang bawk.
Fluorocarbon rubber hi FPM emaw Viton emaw an ti bawk. A structure-ah hian fluorine a awm a. FPM hian lumna sang tak tak leh chemical chak tak tak a tuar thei a ni. Oil, fuel, solvent-ah te a chhe lo. FPM hi car, thlawhna leh factory-a seal leh gasket siamna atan hman a ni. Thil a lum lutuk emaw, chemical na tak tak awmna hmunah emaw a thawk tha hle.
Silicone rubber hi a bendy hle a, lumna sang tak a la thei bawk. Mihring tan a him a, chemical nen pawh a inrem lo. Electronics-ah chuan wire a khuh a, part hrang hrang a seal bawk. Damdawi inah chuan tube, catheter leh implant atan te hman a ni. Silicone rubber hi a chiangin a nem a, chuvangin damdawi leh ha enkawlna hmanrua atan a tha hle.
Polyisoprene hi synthetic rubber a ni a, natural rubber nen a inang hle. Latex protein a neih loh avangin allergy a siam lo. Polyisoprene hi damdawi leh ei leh in atan hman a ni. Siam a awlsam a, ozone emaw chemical emaw-ah a chhe lo. Polyisoprene hi natural rubber angin a stretchy lo a, mahse allergy nei tan chuan a even zawk a, a him zawk bawk.
Santoprene hi rubber bik a ni a, rubber leh plastic ang maiin a thawk bawk. EPDM rubber leh polypropylene chawhpawlh atanga siam a ni. Santoprene hi hman nawn leh theih a ni a, hei hi planet tan a tha hle. Chemical, khaw lum leh bending te pawh a tuar thei. Santoprene hi car seal, hose, leh in lama thil siamah te hman a ni. Appliances leh pawn lam thilah pawh a awm bawk. Santoprene chi thar siam a awlsam zawk a, a man pawh a tlawm zawk.
| Feature/Property | Description | Motor hman dan | Consumer Goods hman dan |
|---|---|---|---|
| Material chi hrang hrang | Santoprene hi EPDM rubber leh polypropylene atanga siam a ni | Car seal, hose, leh car chhung leh pawn lam part siamna atan hman thin | Inchhung bungrua, wire, leh pawn lam thil siamna atana hman thin |
| A chhe thei lo | A khauh hle a, a chhe awlsam lo bawk | Car parts te chu rei zawk a daih tir a, chhiatna a do thei bawk | In chhunga thil awmte chu a chak a, stress tuar thei turin a siam |
| Chemical laka inven theihna | Acid, oil, grease te hian a tichhe lo | Fluid khawih thei car parts tan a tha | Chemical khawih thei inchhung thil atan a tha |
| Khaw lum leh khaw vawt laka inven theihna | Ni leh ruah surah a crack lo | Pawn lama car parts atan hman thin | Pawn lama in lama thil siamna atana hman thin |
| Temperature Range a ni | A lum em em atanga a lum em em thlengin a thawk thei | Car air system leh hose-ah te hman thin | Appliances lum leh vawt tan a tha |
| Recycle theihna a ni | Recycle leh hman leh theih a ni | Car siamtute chu green zawka awm turin a pui | Environment tan a tha |
| Processability leh Surface Quality a ni | Santoprene thar hi a siam a awlsam a, a hmel pawh a mawi hle | Car part hrang hrang, a hmel leh a rilru a hahdam ngai te tan hman a ni | In chhunga thil awmte chu a flexible leh mawi takin a siam |
| Aesthetic leh Functional Quality te a awm bawk | Strong, bendy, leh hmeltha tak a ni | Car chhung leh panel atan hman a ni | In lama thil tough leh hmeltha tur atana hman thin |
Santoprene hi car leh in lama bungrua atan chuan top choice a ni a, a chhan chu a chak a, a flexible bawk.
Buna rubber-ah hian Buna-N leh Buna-S te a tel. Buna-N hi acrylonitrile leh butadiene atanga siam a ni. Oil leh fuel do kawngah a tha hle. Buna-S hi styrene leh butadiene atanga siam a ni. Khua lum leh chemical lakah a ding thei. Buna-N hi seal leh hose atan hman a ni. Buna-S hi tyre, belt, leh pheikhawk kekawr ah te hman a ni. Factory te hian heng rubber te hi mamawh hrang hrang nena inmil tura siam dan hi an thlak danglam thei a ni.
Ethylene propylene rubber, a nih loh leh EPM hi synthetic rubber a ni a, a hnungzang chu a nghet hle. Khua lum, ni, leh khaw lum vangin a chhe lo. EPM hi khaw lum lai pawhin a bendy reng a, electric tihtawp nan a tha hle. Car kawngkhar, hose, inchung leh cable-ah te hman a ni. EPM hi a tough a, flexible tak a nih avangin car leh building-ah pawh a thawk tha hle.
Epichlorohydrin rubber hian oil, fuel, leh chemicals te a do tha hle. Hmun harsa takah a chakna a vawng reng a, gas a kal tlang tir lo. CO rubber hi car leh thlawhnaah fuel hose, seal, leh gasket siam nan an hmang thin. Khua lum leh vawt ah pawh a thawk a, a bend tha hle. CO rubber hi metal leh fabric-ah a innghat tha hle a, hei hian seal nghet tak siam a pui thin.
Tip: Rubber chi khat i thlan dawnin i mamawh tur ngaihtuah la. Temperature dik tak, chemical leh a ben theih zat dik tak a tuar thei em tih enfiah rawh.
Abrasion resistance tih awmzia chu rubber hian rubbing a tuar thiam em em tihna a ni. Hemi kawngah hian Nitrile rubber leh styrene-butadiene rubber te hi an thiam hle. Nitrile rubber hi car hose, fuel line, O-ring, leh seal-ah te hman a ni. A chhe rang lo va, oil pawh a tuar thei bawk. Styrene-butadiene rubber hi tire, pheikhawk kephah, belt leh floor atan an thlang thin. Factory-ah pawh polyurethane hi a chhe thei lo bawk. Neoprene leh Viton hian hna tha tak thawk mahse Nitrile emaw SBR emaw angin an thawk tha lo. EPDM leh silicone hian wear a do thei lo va, hna rough tak tak tan pawh a tha ber lo.

| Elastomer | Abrasion Resistance | A hmanna pawimawh tak tak |
|---|---|---|
| Nitrile (NBR) a ni. | A tha lutuk | Motor hose, fuel line, O-ring, gasket, seal te a awm bawk |
| Styrene-Butadiene (SBR) hmanga siam a ni. | A tha lutuk | Motor tire, pheikhawk kephah, conveyor belt, industrial flooring te a awm bawk |
| Polyurethane hmanga siam a ni | A tha lutuk | Industrial application-ah chuan wear resistance sang tak mamawh a ni |
| Neoprene a ni | Tha | A hmanna tlangpui, NBR, SBR, Polyurethane aiin a tlem zawk |
| Viton chuan a rawn ti a | Tha | Aerospace seal, chemical leh fuel hman dan tur |
| EPDM a ni | Dik | Abrasion-critical hmanna atan a tha lo zawk |
| Silicone hmanga siam a ni | Dik | Temperature sang, abrasion resistance tha lo |
Synthetic rubber thenkhat chuan oil leh chemical te chu an handle tha hle. Nitrile butadiene rubber hi oil, fuel, leh grease te nen a tha hle. Viton hi chemical chak tak tak leh oil nen a tha zawk. Hei hian thlawhna leh chemical plant tan a tha hle. Neoprene hi a chak a, oil leh chemical te pawh a tuar thei bawk. Gloves, wetsuit, leh seal-ah te hman a ni. Heng rubber te hian leak a titawp a, car, thlawhna leh ei tur siamna hmuna machine te chu him takin a vawng reng bawk.
NBR hian oil, fuel, acid, base, leh cleaner te a hmachhawn thei a ni.
Viton hian chemical khauh tak tak leh lumna sang tak hmangin hna a thawk thin.
Neoprene hi hna tam takah thlan a ni a, a chhan chu a chak a, oil a do thei bawk.
Rubber, khaw lum leh khaw lum do thei tur chu pawnah leh hmun lum lamah a mamawh a ni. EPDM rubber hi ni, ozone, ruahsur vangin a chhe lo. Car seal, roof, leh pawn lama hose siamna atan hman a ni. Silicone rubber hi a nem reng a, a pianzia chu lumna sang takah a vawng reng a, 572°F thleng a ni. Viton hi hmun harsa takah a tha a, heat leh chemicals te pawh a handle thei. Heng rubber te hi motor, factory leh building-ah te, khaw lum leh khaw vawt hian harsatna a thlen theihna hmunah te an hmang thin.
EPDM hi pawn lam seal leh roof atan a tha ber.
Silicone hi oven gasket, damdawi hmanrua, leh electronics-ah te hman a ni.
Viton hi thlawhna leh chemical plant atan thlan a ni.
Rubber thenkhat chu a dang aiin gas block thiam zawk an ni. Butyl rubber hian boruak a paltlang loh nan a veng a, chuvangin tire tube leh liner-ah te hman a ni. Epichlorohydrin rubber hian gas pawh a block tha hle a, fuel system-ah pawh hman a ni. EPDM hi gas tihtawp nan a tha hle a, a bik takin steam leh brake part-ah te a tha hle.
| Synthetic Rubber | Gas a luh theih lohna ziarang | A hmanna ber |
|---|---|---|
| Butyl Rubber hmanga siam a ni | Gas-te laka inpermeability sang tak; thermal expansion hniam tak a ni | Tire chhunga tube, tyre liner, sidewall te a awm bawk |
| Epichlorohydrin (ECO) hmanga siam a ni. | Nitrile nena khaikhin chuan gas impermeability sang zawk | Fuel system hrang hrang a awm bawk |
| EPDM a ni | High-temp water vapor atan a tha | Steam, brake system part hrang hrangte tan seal a awm |
Rubber thenkhat chu hna bik atan an pickup thin. Neoprene hi tubing, wire khuhna, leh himna thawmhnaw atan te hman a ni. Nitrile rubber hi oil hose-ah te, fuel tank-ah te, rocket part-ah te pawh hman a ni. Hydrogenated NBR hian boruak a ti chhuak tha hle. Butyl rubber hian gas a tikhawlo thei a, electric a titawp thei bawk. EPDM hi car part leh pheikhawk siamnaah hman a ni a, a chhan chu khaw lum a tuar thei a ni. Urethane elastomer hi spandex ang chi hi thil stretchy leh airplane wheel-ah te hmuh tur a awm a. Silicone rubber hian temperature tam takah hna a thawk a, wire khuhna atan hman a ni.
Santoprene hi bendy leh tough tia hriat a ni. Factory-te chuan santoprene hi car seal-ah te, hose-ah te, in lama machine-ah te, leh pawn lam thil siamnaah te an hmang thin. Santoprene hi awlsam taka recycle leh shaped theih a nih avangin car leh home goods atan chuan top pick a ni. Vulcanization hian santoprene hi a tichak a, a daih rei bawk a, chuvangin hmun harsaah pawh hna a thawk thin. Vulcanization hian santoprene hi hman leh theih a ni bawk a, hei hian planet hi a pui hle.
Tip: Hnathawh tur rubber dik tak thlang fo ang che. Bendy seal atan santoprene hmang la, oil atan NBR hmang la, pawn lama hman atan EPDM hmang bawk ang che.
A hnuaia table hian synthetic rubber chi hrang hrang tehkhin nan a pui a ni . An perform dan, eng chen nge an awm tih leh engzat nge an sen tih a tarlang a ni. Hei hian hna tin atan eng chi nge tha ber tih hriat a awlsam phah hle.
| Type | Key chakna | Durability | Cost Level | Hman dan tlangpui |
|---|---|---|---|---|
| SBR | Abrasion resistance tha tak, siam awlsam | Thunun | Hniam | Tyre, pheikhawk hnuai lam, belt te |
| NBR | Oil leh fuel a do thei a, a chak | A hniam lam (UV/ozone tha lo) . | Hniam | Seal, hose, fuel system te a awm bawk |
| EPDM a ni | Weather, UV, leh chemicals te a buaipui thin | Sang | Thunun | Car seal, roofing, pawn lam parts te pawh a awm bawk |
| Neoprene (CR) hmanga siam a ni. | Oil, chemical leh khaw lum leh khaw vawt a do thei | Thunun | Thunun | Gasket, wetsuit, belt te pawh a awm bawk |
| Butyl (IIR) a ni. | Thli a luh tir a, gas a block bawk | A sang (oil/ozone tha lo) 1.1. | Thunun | Tyre tube, seal, stopper te pawh a awm bawk |
| Silicone hmanga siam a ni | Heat, cold, leh UV te a handle | Sang | Sang | Damdawi lam, electronics, chhang siamna |
| Fluorocarbon (FKM) hmanga siam a ni. | Chemical na tak leh lumna a do thei | Sang | Sang | Aerospace, chemical chi hrang hrang siamna hmun |
| Polyurethane (PU) hmanga siam a ni. | Wear and tear laka chak tak a ni | A hniam lam (UV/ozone tha lo) . | Moderate-High a ni | Wheel, bushing, machinery te pawh a awm bawk |
Note: Synthetic rubber hi hna bik atan siam theih a ni. A chi thenkhat chu hmun harsaah chuan rei zawk an daih. Mi dangte chuan an man a to zawk emaw, oil hmangin hna an thawk tha zawk emaw.
dik tak thlan Synthetic rubber chu i mamawh danah a innghat. I duhthlanna atana ṭanpui thei tur step ṭhenkhat chu hetiang hi a ni:
Environment enfiah : Khua lum, vawt, ni, chemical emaw a hmachhawn dawn em ni? Pawn lam atan EPDM emaw silicone emaw hmang rawh. Oil emaw fuel emaw atan NBR thlang rawh.
Chakna ngaihtuah : A insiamrem emaw, nghet taka awm emaw a ngai em? Polyurethane hi a tough a, a chhe rang lo. Silicone hi khaw lum leh vawt ah pawh a bendy reng thin.
Look at cost : SBR hi a man tlawm a, thil tam takah a thawk thei. Silicone leh fluorocarbon hi a man a to zawk a, mahse hmun harsa takah chuan rei zawk a daih thung.
Match the use : SBR leh butyl rubber te hi tyre atan hman a ni. Silicone hi damdawi leh ei leh in hna atan a him. Engine seal atan NBR emaw fluorocarbon emaw a tha.
Dan leh himna enfiah : Hna thenkhatah chuan himna dan zawm tur rubber a ngai. Type approved a nih leh nih loh enfiah fo ang che.
awm . Synthetic rubber chi hrang hrang thlan tur a Hna hrang hrang atan feature bik an nei vek a ni. Hnathawh tur, a hmanna tur hmun leh budget ngaihtuah hian i project atana rubber tha ber i thlang thei ang.
Synthetic rubber chi hrang hrang hi a inang vek lo. Ṭhenkhat chu a dang aiin an chak zawk emaw, an bendy zawk emaw a ni. Ṭhenkhat chuan khaw lum, oil, a nih loh leh boruak ṭha lo chu an tuar thiam zawk. Type dik thlan hian thil a daih rei a, a thawk tha bawk. He table hian siamtute chu hna tin atan rubber tha ber thlang turin a pui a:
| Type | Key Properties | Best Uses |
|---|---|---|
| NBR | Oil leh fuel laka inven theihna | Engine seal, hose te a awm bawk |
| EPDM a ni | Khaw lum leh khaw vawt laka inven theihna | Roofing, car seal te pawh a awm bawk |
| Neoprene a ni | Chemical leh kangmei laka inven theihna | Wetsuit, gasket te pawh a awm bawk |
| Silicone hmanga siam a ni | Heat sang leh flexibility sang tak a ni | Damdawi lam, chaw ei tur bungrua |
| Viton chuan a rawn ti a | Chemical leh temperature laka invenna nasa tak a nei | Aerospace, O-ring te pawh a awm bawk |
Santoprene hi car leh in lama thil siamah chuan bendy leh tough tak a nih avangin hriat a ni.
Natural rubber hi thing atanga lo chhuak a ni. Synthetic rubber hi factory-ah oil chemical atanga siam a ni. Synthetic rubber hi hna bik atan thlak theih a ni. A chi hnih hian an inzawm khawm thei a, an pianziaah an kir leh thei bawk. Synthetic rubber hi hmun khauh takah a rei zawk tlangpui.
Car tyre atan Styrene-butadiene rubber (SBR) leh butadiene rubber (BR) te hi a tha ber. An chhe chak lo va, lumna an la thei bawk. Tyre siamtute chuan SBR chu natural rubber nen an pawlh a, tire chu a chak zawk a, rei zawk a daih thei bawk.
Ni e, synthetic rubber chi hrang hrang hi recycle theih a ni. Santoprene hi recycle a awlsam hle. Recycling hian bawlhhlawh tihtlem a pui a, bungrua a humhim bawk. Recycled rubber ṭhenkhat chu car part thar siamna atan, floor thar atan emaw, inkhelhna hmun atan emaw hman a ni.
Nitrile (NBR) leh fluorocarbon (Viton) te hian chemical makeup bik an nei a. Hengte hian oil leh chemical te hian rubber a ti na lo. Chuvang chuan engine leh factory-a seal, hose leh gasket atan te an tha hle.
Awle, silicone rubber hi ei leh in leh damdawi lam thil atan a him. Chemical tam zawk nen a inrem lo va, lumna sang tak a la thei bawk. Hospital-ah chuan tube leh implant atan silicone an hmang thin. Chaw siamtute chuan baking mat leh kitchen hmanrua atan an hmang thin.