GA-57XX
Herchy
| kasedhiyan: | |
|---|---|
| Jumlah: | |
Aplikasi: cocok kanggo ngasilake hot stamping cots, hot stamping plate, panas transfer roller, copier roller, etc.
Fitur utama: resistance banget kanggo suhu dhuwur lan kurang (60 'C -350 'C), ketahanan dhuwur lan resistance abrasion apik, kurang deformasi pesawat, hard kanggo deformasi lan fraktur, umur layanan dawa.
Pengujian: 1% agen curing (50% tempel DBPMH ing permen karet silikon),175'C x 5min x 15MPa.
| Parameter produk | ||||||
| produk | GA-5750 | GA-5770 | GA-5780 | GA-5741 | GA-5761 | |
| Penampilan | hory | Fat kuning | ||||
| Kekerasan (ShoreA) | 55 | 70 | 80 | 43 | 60 | |
| Kekuatan tarik (MPa) | 5.5 | 6 | 7 | 6 | 8 | |
| Elongasi (%) | 230 | 150 | 100 | 400 | 350 | |
| Kekuwatan sobek (kN/m) | 10 | 9 | 9 | 15 | 25 | |
| 175'C x22h Kompresi(%) | 8 | 10 | 10 | 10 | 10 | |