Tel: +86 15221953351 . info@herchyrubber.com
Please Choose Your Language
Nā huahana
Aiaʻoe: KA HOME » Nā huahana » Synthesis Rubber » VMQ Silneno » Ga-93x0 iā ia iho me ka libricating silicone silicone silicone (silicated silica) (hcr)

KAUIHOA

Kaʻana like:
ʻO ke pihi Sharing Charing
Twitter Sharing
laina kaʻa kaʻa kaʻa
ʻO ka pihi Wechat Sharing
ʻO ke pihi kaʻana Linkedin
Ke kaʻanaʻo Pinterest Baring
ʻO ka pihi kaʻaheleʻo Whatsapp
ʻO ka pihi Sharings Sharing

Ga-93x0 pilikino pono'ī silicone silicone silicone silber (silicated silica) (hcr)

Ke noi: He kūpono no ka hanaʻana o ka hōʻailonaʻana i nā huahana a me nā huahana'ē aʻe.
ʻO ka hiʻohiʻona nui:ʻO ka waiwai momona maikaʻi,ʻoi aku ka nui o nā waiwai o ka aila ma luna o 7%, e hele i ka mea i loaʻa i nā rohs a hiki aku.
  • GO-93x0

  • Herchy

Loaʻa:
Ka nui:

Hōʻike: 1% o nā Agent Curing (50% Paste o DBPMH Institute 小 COEGGUM), 175 ° C x 5mpa.


Nā waihona huahana
'Ōpilo Froper Ga-9330 GE-9340 GE-9350 Ga-9360 GE-9370
Helehelena Milywhite milywhite
VidiamplaticSity 140 170 200 220 240
Paʻakikī (shoerea) 30 40 50 60 70
Density (g / cm3) 1.12 1.14 1.17 1.2 1.21
Ikaika ikaika (MPA) 9 10 10 8.5 8.5
Elongation (%) 850 800 700 500 350
Ka ikaika o ka make (kn / m) 20 25 30 25 25


MAUI: 
Akahi: 

Nā loulou wikiwiki

ʻO kā mākou huahana

Hoʻokaʻaʻikeʻike

Add: No.33, HELE 159, Tai Makey, Tai Makex, Hangki
Tel / Whatsapp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Ke kulekele | Kākoʻo Noeli Leikahi.