GA-91X0
Herchy
| Loaʻa: | |
|---|---|
| Nui: | |
Ho'āʻo: 1% o ka lāʻau lapaʻau (50% paʻi o DBPMH i ka silicone gum), 175° x5minx15MPa
| Nā palena huahana | |||||
| Huahana | GA-9130 |
GA-9140 | GA-9150 | GA-9160 | GA-9170 |
| Ka nana aku | Alohilohi | ||||
| Williamplasticity |
150 |
190 |
250 |
280 |
300 |
| Paʻakikī (ShoreA) |
30 |
40 |
50 |
60 |
70 |
| Māmā (g/cm3) | 1.11 |
1.14 |
1.17 |
1.20 |
1.21 |
| Ka ikaika uʻi (MPa) |
8.0 |
9.5 |
10.0 |
9.0 |
8.5 |
| Elongation(%) | 900 |
700 |
600 |
500 |
400 |
| Kaha waimaka (kN/m) | 17 |
20 |
25 |
25 |
25 |
| Ke kū'ē i luna (Ω) | 1011 |
||||