FV9600
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
Items |
Index |
||
Giredhi |
FV9660 |
FV9670 |
|
Chitarisiko Miedzo Nzira |
Chena |
||
Chaiyo Gravity/g/cm3 |
ASTM D792 |
1.46 |
1.48 |
Huoma/mahombekombeA |
ASTM D2240 |
60 |
70 |
Tensile Simba/MPa |
ASTM D412 |
6.8 |
6.5 |
Elongation Panguva Yekuzorora /% |
ASTM D412 |
310 |
290 |
Kusimba Kwemisodzi/KN/m |
ASTM D624-B |
17 |
17 |
* Heat Resistance |
Huoma shanduko/mahombekombe A |
+5 |
+5 |
Kuchinja kwesimba rekusimba,% |
3.8 |
3.5 |
|
Kuchinja kwesimba rekusimba,% |
161 |
154 |
|
IRM903 |
ASTM D471 |
5.5 |
5.2 |
Mafuta C |
ASTM D471 |
20 |
20 |
Murazvo-retardant Level |
GBT10707-2008 |
FV 0 |
FV 0 |
Curing Condition |
Wedzera 0.7 zvikamu zvebis(2+5), imwe nhanho vulcanisation 170 ℃×15min, maviri nhanho vulcanisation: 200℃×4h. |
||