FV9600
Herchy
| Kasadiaan: | |
|---|---|
| Kuantitas: | |
Barang |
Indéks |
||
Kelas |
FV9660 |
FV9670 |
|
Penampilan Métode Tés |
Bodas |
||
Gravitasi spésifik/g/cm3 |
ASTM D792 |
1.46 |
1.48 |
Teuas / basisirA |
ASTM D2240 |
60 |
70 |
Kakuatan Tensile / MPa |
ASTM D412 |
6.8 |
6.5 |
Elongation dina putus /% |
ASTM D412 |
310 |
290 |
Kakuatan cimata / KN / m |
ASTM D624-B |
17 |
17 |
* Résistansi Panas |
Parobahan karasa / basisir A |
+5 |
+5 |
Parobahan kakuatan tensile,% |
3.8 |
3.5 |
|
Parobahan kakuatan tensile,% |
161 |
154 |
|
IRM903 |
ASTM D471 |
5.5 |
5.2 |
Suluh C |
ASTM D471 |
20 |
20 |
Tingkat seuneu-retardant |
GBT10707-2008 |
FV 0 |
FV 0 |
Kaayaan Curing |
Tambahkeun 0,7 bagian bis (2 + 5), hiji tahap vulkanisasi 170 ℃ × 15min, dua tahap vulkanisasi: 200 ℃ × 4h. |
||