FV9600 we gɛt fɔ du wit am
Herchy na di .
| Avaylabl: | |
|---|---|
| Kwantiti: | |
Tin dɛn |
Index |
||
Mak |
FV9660 we de na di wɔl |
FV9670 we de na di wɔl |
|
Aw a luk Di We dɛn fɔ Tɛst |
Wayt |
||
Spesifi k Graviti/g/cm3 |
ASTM D792 we yu de yuz |
1.46 |
1.48 |
Hadnɛs/shɔA |
ASTM D2240 we yu de yuz |
60 |
70 |
Tensile Strɔng/MPa |
ASTM D412 we yu kin yuz |
6.8 |
6.5 |
Elongation Na Brek /% . |
ASTM D412 we yu kin yuz |
310 |
290 |
Tiar Strɔng/KN/m |
ASTM D624-B we yu de yuz |
17 |
17 |
*Hɛt rɛsistɛns |
Hadnes chenj /sho A |
+5 |
+5 |
Tensile trɛnk chenj, % . |
3.8 |
3.5 |
|
Tensile trɛnk chenj, % . |
161 |
154 |
|
IRM903 |
ASTM D471 we yu kin yuz |
5.5 |
5.2 |
Fiul C |
ASTM D471 we yu kin yuz |
20 |
20 |
Level we nɔ de mek faya |
GBT10707-2008. Di wan dɛn we de wok |
FV 0. Di wan dɛn we de wok |
FV 0. Di wan dɛn we de wok |
Di Kɔndishɔn we de mɛn am |
Ad 0.7 pat pan bis(2+5), wan stej vulkanayzeshɔn 170°C×15min, tu stej vulkanayzeshɔn: 200°C×4h. |
||